INSULCURE 11B

Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission

INSULCURE 11B

Main features

  • Heat-Curing INSULCAST Epoxy Curing Agent
  • 700 cP Application Viscosity
  • 3-Hour 100 deg C Cure

Product Description

INSULCURE® 11B Epoxy Curing Agent is a rigid, temperature-resistant, heat-curing agent for compatible INSULCAST epoxy casting and encapsulation resins. The amber liquid is selected when extended pot life and elevated-temperature cured performance are required. Current supplier information lists a typical viscosity of 700 cP, a 300-minute pot life in the referenced system, and a three-hour cure schedule at 100°C. Final mix ratio and cured properties depend on the specific INSULCAST resin, so this component should be presented and processed only as part of a verified resin-hardener system.

Key features

  • Heat-curing epoxy hardener: The curing agent is intended for compatible INSULCAST resin systems.
  • Extended process window: Current supplier information lists a 300-minute pot life in the referenced system.
  • Temperature-resistant rigid cure: The product is positioned for elevated-temperature epoxy systems.

Applications / Suitable for

  • Curing compatible INSULCAST epoxy resins
  • Heat-cured electrical potting systems
  • Temperature-resistant epoxy casting systems
Product Family

INSULCURE 11B

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Component role Epoxy curing agent N/A As supplied
Appearance Amber liquid N/A Product family description
Viscosity 700 cP Current supplier product page
Pot life 300 min Referenced system at 25°C
Reference cure 3 h At 100°C