INSULGEL 70 CC

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

INSULGEL 70 CC

Main features

  • Low-Shrinkage Thermal-Shock-Resistant Epoxy
  • Three Curing-Agent Options
  • Shore D 43 to 80 Hardness

Product Description

INSULGEL® 70 CC Black Epoxy Compound is a black, semi-flexible epoxy potting and encapsulation compound formulated for low shrinkage, low coefficient of thermal expansion, and thermal-shock resistance. The base resin may be combined with Part B-1, INSULCURE 9, or INSULCURE 11B to provide different pot life, cure, hardness, and service-temperature profiles. Typical base viscosity is 16,000 cP at 25°C. Depending on the curing agent, the cured system provides Shore D 43 to 80 hardness, 20% to 120% elongation, and service from -40°C to 155°C.

Key features

  • Semi-flexible low-stress epoxy: The formulation is documented for reduced shrinkage and thermal-shock resistance.
  • Three curing-agent options: Part B-1, INSULCURE 9, and INSULCURE 11B provide different processing windows.
  • Hardener-dependent flexibility: Typical cured elongation ranges from 20% to 120%, depending on the curing agent.

Applications / Suitable for

  • Thermal-shock-resistant potting
  • Low-stress electrical encapsulation
  • Assemblies requiring improved component adhesion
Product Family

INSULGEL 70 CC

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Base color Black N/A INSULGEL 70 CC
Base viscosity 16,000 cP At 25°C
Base specific gravity 1.53 N/A At 25°C
Mix ratio with Part B-1 100:9 to 10 parts by weight Base : hardener
Mix ratio with INSULCURE 9 100:3.5 to 4 parts by weight Base : hardener
Mix ratio with INSULCURE 11B 100:8 parts by weight Base : hardener
Pot life 0.5 to 10 h Depending on curing agent at 25°C
Shelf life 12 months All components
Technical properties

After-processing / final-state properties

Typical cured or final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Hardness 43 to 80 Shore D Depending on curing agent
Tensile strength 7 to 17 MPa Depending on curing agent
Tensile elongation 20 to 120 % Depending on curing agent
Coefficient of thermal expansion 64 to 70 × 10⁻⁶ 1/°C Depending on curing agent
Thermal conductivity 0.52 to 0.62 W/m·K Converted from published values
Service temperature -40 to 155 °C Depending on curing agent
Dielectric strength 400 to 425 V/mil Depending on curing agent
Volume resistivity 7 × 10¹² to 1 × 10¹⁵ ohm·cm At 25°C, depending on curing agent