FM-0421 | Reactive PDMS - Monoterminal Hydroxy
Harmonization Code : 3910.00.00.60 | Polydimethylsiloxane, whether or not polyethylene glycol and trifluoropropyl substituted, with methacrylate end groups
Main features
- Mono terminal
- 5,000 g/mol | 70 mPas
- Hydroxy functional group
Product Description
Silaplane® FM-0421 is a reactive polydimethylsiloxane (PDMS) based polymer with a molecular weight of 5,000 g/mol and a Viscosity of 60-80 mPas. This reactive silicone material offers the addition of silicone-type properties to non-Silicone materials in a variety of industries including electronics, semiconductors, automotive, biotech, healthcare, and clean energy applications. It offers narrow polydispersity and a low level of chemical impurities.
Silaplane® FM-0421 mono-terminal product has a Hydroxy functional group that is reactive toward a variety of compounds and surfaces enabling chemical and physical changes to chemicals, particle surfaces and larger surface structures. Hydroxy groups are mainly reacting with Urethane and Ester compounds. The reactive functional group improves the adsorption to the filler surface and makes the inorganic filler easier to blend into the silicone binder resin. At the same time it displays high affinity for the silicone binder resin which improves the wettability between the filler and the binder. This product stabilizes the filler dispersion due to the repulsive force between fillers, achieved by silicone repulsion and the osmotic pressure effect.
Product Benefits:
- Filler dispersion stabilization with low viscosity
- Water/Oil repellency
- Gas permeability (Oxygen, CO2, CH4, etc.)
- Mold releasability
- Anti-Abrasion resistance, Anti-fouling