FM-4411 | Reactive PDMS - Bi terminal Hydroxy
Harmonization Code : 3910.00.00.60 | Polydimethylsiloxane, whether or not polyethylene glycol and trifluoropropyl substituted, with methacrylate end groups
Main features
- Bi terminal
- 1,000 g/mol | 35 mPas
- Hydroxy functional groups
Product Description
Silaplane® FM-4411 is a reactive polydimethylsiloxane (PDMS) based polymer with a molecular weight of 1,000 g/mol and a Viscosity of 30 - 40 mPas. This reactive silicone material offers the addition of silicone-type properties to non-Silicone materials in a variety of industries including electronics, semiconductors, automotive, biotech, healthcare, and clean energy applications. It offers narrow polydispersity and a low level of chemical impurities.
Silaplane® FM-4411 bi-terminal product has two Hydroxy functional groups that are reactive toward a variety of compounds and surfaces enabling chemical and physical changes to chemicals, particle surfaces and larger surface structures. Hydroxy groups are mainly reactive with urethane and ester compounds.