JNC PA-1210-020 | Insulating Polyacrylate Ink
Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category
Main features
- UV Curable/ Solvent free
- Standard
- Optoelectronics
Product Description
PA-1210-020 is a UV-curable, solvent-free polyacrylate insulating ink. Its advanced polyacrylate composition ensures robust dielectric properties of a breakdown voltage of 100 V/um and a dielectric constant of 3.2 @ 1 kHz, ensuring dependable electrical isolation and signal integrity for your components. Moreover, with its solvent-free formulation, PA-1210-020 contributes to a safer and more environmentally friendly production process, minimizing volatile organic compounds (VOCs) and reducing the ecological footprint.
Industry Applications:
Electronics Manufacturing | Optoelectronics | Microelectronics
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Electrical Properties
Mechanical Properties
Chemical Properties
Physical Properties
Additional Information
| Properties | PA-1210-020 |
| Solids content (wt. %) | 100 |
| Viscosity (mPa's) @25℃ | 23 |
| Surface tension (mN/m) @23℃ | 30 |
| Printing methods | Inkjet |
| Curing | 2,000mJ/cm2 @ 365nm |
| Post-curing | 175℃ 60min |
| Volume resistivity (Ω*cm) | 1E+16 |
| Breakdown voltage (V/um) | 100 |
| Dielectric constant (1kHz) @1V | 3.2 |
| Tensile modulus (MPa) | 1800 |
| Elongation (%) | 3 |
| Residual stress (MPa) | 12 |
| 5% weight loss temp (℃) | 275 |
| CTE ( | 55 |
| Tg (℃) | 116 |
| Water absorbance (%) @23℃ | 0.2 |