JNC PA-1210-035 | Insulating Polyacrylate Ink
Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category
Main features
- UV Curable/ Solvent free
- High Insulation reliability for thin film devices
- Optical Devices
Product Description
PA-1210-035 is a UV-curable, solvent-free polyacrylate insulating ink. With its advanced polyacrylate technology, this ink strikes a perfect balance between flexibility and durability. Components coated with PA-1210-035 gain structural integrity capable of withstanding both mechanical stress and temperature fluctuations.
PA-1210-035 rapidly cures under UV light, creating a high-performance insulating layer that not only ensures reliable results but also speeds up your production process. Boasting an ultra-low water absorbance of less than 0.1%, this ink confidently resists moisture-induced vulnerabilities, ensuring consistent performance in humid conditions.
Industry Applications:
Thin Film Electronics | Microfabrication | Optical Devices
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Electrical Properties
Mechanical Properties
Chemical Properties
Physical Properties
Additional Information
| Properties | PA-1210-035 |
| Solids content (wt. %) | 100 |
| Viscosity (mPa's) @25℃ | 36 |
| Surface tension (mN/m) @23℃ | 31 |
| Printing methods | Inkjet |
| Curing | 2,000mJ/cm2 @ 365nm |
| Post-curing | 175℃ 60min |
| Volume resistivity (Ω*cm) | 6E+16 |
| Breakdown voltage (V/um) | 100 |
| Dielectric constant (1kHz) @1V | 3.1 |
| Tensile modulus (MPa) | 1400 |
| Elongation (%) | 3 |
| Residual stress (MPa) | 19 |
| 5% weight loss temp (℃) | 292 |
| CTE ( | 76 |
| Tg (℃) | 126 |
| Water absorbance (%) @23℃ | <0.1 |
Recommended Cleaner usage: 3 times the ink volume