KESTER 2235 Soldering Flux
Harmonization Code : 29051200 | Propan-1-ol (propyl alcohol) and propan-2-ol (isopropyl alcohol)
Main features
- Minimizes icicling and bridging
- Compatible with most masks and laminates
- High activity
Product Description
KESTER 2235 is a high activity 11% solids organic flux designed for automated soldering of circuit board assemblies where a more aggressive flux is required, but reliability considerations are paramount. 2235, a flux with comparably low solids in respect to other fluxes in the same category, will produce fewer skips on the bottom side surface mount pads. The residue after soldering is effectively removed in standard water cleaning systems. Although possessing high activity, boards exhibit high ionic cleanliness after water cleaning, exceeding the requirements of MIL-P-28809. No offensive odors or excessive smoke are emitted during soldering. The flux will not create excessive foaming in standard water cleaning systems. 2235 is classified as ORH1.
Product Key Features
- Minimizes icicling and bridging
- Chemically compatible with most masks and laminates
- High activity
- Classified as ORH1.
Applications
- Highly recommended for surface mount PCBs.
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
Flux Application
2235 can be applied to circuit boards by a spray, foam or dip process. An air knife after the flux tank is recommended to remove excess flux from the circuit board and prevent dripping on the preheater surface