LAIRD RFLB/SS6M
Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other
Main features
- Adhesive-Backed 0.51 mm Sheet
- 10 MHz to 4 GHz Control
- Greater Than 50 dB/cm Attenuation
Product Description
Eccosorb RF-LB RFLB/SS6M EMI Noise Suppression Absorber is a 0.51 mm grey silicone sheet with SS6M pressure-sensitive adhesive for localized low-frequency noise control. The configured 304.8 x 914.4 mm part covers 10 MHz to 4 GHz and has typical attenuation greater than 50 dB/cm at 2.5 GHz. Its flexible format supports placement over processors, memory, power ICs, circuit traces, flat cables, displays, and other radiating structures. Applications include control of surface currents, crosstalk, radiated emissions, unwanted coupling, and lower-microwave cavity resonances.
Key features
- Thin Adhesive-Backed Placement: The 0.51 mm sheet uses an SS6M pressure-sensitive adhesive for localized installation.
- Broad Low-Frequency Coverage: The configured absorber covers a documented 10 MHz to 4 GHz frequency range.
- High Attenuation at 2.5 GHz: Typical attenuation is greater than 50 dB/cm at the stated frequency.
Applications / Suitable for
- Processors, chipsets, memory, and power ICs
- Circuit traces, high-speed lines, and flat cables
- Surface-current, crosstalk, emission, and cavity-resonance control
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
As-supplied construction, dimensions, and handling properties for the RFLB/SS6M 0.020 x 12 x 36 inch configuration.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Resin system | Silicone | Configured RF-LB part | |
| Color | Grey | Visual | |
| Thickness | 0.51 | mm | Configured part |
| Sheet size | 304.8 x 914.4 | mm | Configured part |
| Density | 2.20 | g/cc | Typical property |
| Hardness | 70 with a tolerance of 10 | Shore A | Typical RF-LB data |
| Adhesive option | SS6M PSA | Configured part | |
| Shelf life | Minimum 365 | days from shipment | Typical property |
After-processing / final-state properties
Typical electromagnetic, electrical, temperature, and outgassing properties for the configured RF-LB absorber; attenuation depends on frequency and installation.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Frequency range | 10 MHz to 4 GHz | Configured part | |
| Attenuation at 2.5 GHz | Greater than 50 | dB/cm | Typical property |
| Permeability at 1 MHz | 40 | Typical property | |
| Operating temperature | -70 to 177 | deg C | Typical property |
| Volume resistivity | 7.45 x 10^11 | ohm cm | Typical property |
| Outgassing TML | 1.150 | % | Typical property |
| Outgassing CVCM | 0.120 | % | Typical property |
| Flammability | UL 94 H-B | Configured part |