ITO-125 | 125 μm Indium Tin Oxide film
Harmonization Code : 3920.99.28.90 | Other plates, sheets, film, foil and strip, of plastics, non-cellular and not reinforced, laminated, supported or similarly combined with other materials ; Of other plastics ; Other; Other
Main features
- 85% Light transmittance
- 125um thickness
- Ease of processing
Product Description
LINQTAPE ITO-125 is a transparent 125μm film made out of Indium Tin Oxide (ITO) backed on a PET substrate. ITO-125 is a n-type semiconductor material, which offers a unique combination of properties that are useful for a wide range of applications.
LINQTAPE ITO-125 has exceptional high visible light transmittance and low resistivity, making ITO conductive film one of the most versatile and high-performance conductive materials available. It empowers innovation across industries, and serves as a vital component in touchscreen displays, solar panels, and other cutting-edge technologies.
Applications:
- Flat panel display devices: With exceptional light transmittance of up to 85%, our ITO Conductive Film guarantees crystal-clear visibility within the visible spectral region.
- Solar cells: The layers ensure long-lasting performance even in challenging environments and boast superior ultraviolet (UV) absorption, with an absorption rate exceeding 85%, this film offers excellent UV protection.
Packaging
TDS, SDS & Technical Documents
Technical Specifications
Electrical Properties
Additional Information
Indium Tin Oxide films Feature:
- Outstanding Electrical Conductivity: Achieving impressively low resistivity of up to 10^-4Ω∙cm, this film ensures efficient electrical conductivity for various applications.
- High Visible Light Transmittance: With exceptional light transmittance of up to 85%, our ITO Conductive Film guarantees crystal-clear visibility within the visible spectral region.
- UV Absorption: Boasting superior ultraviolet (UV) absorption, with an absorption rate exceeding 85%, this film offers excellent UV protection.
- Infrared Reflectivity: With an infrared (IR) reflectivity exceeding 80%, it efficiently manages heat and radiation, making it suitable for diverse applications.
- Microwave Attenuation: Our ITO Conductive Film excels in microwave attenuation, with an attenuation rate of up to 85%, making it an ideal choice for applications requiring interference reduction.
- Exceptional Durability: The thin layer exhibits high hardness, wear resistance, and chemical corrosion resistance, ensuring long-lasting performance even in challenging environments.
- Ease of Processing: This film offers excellent machining performance and is easy to etch, allowing for effortless customization to meet your specific requirements.