LE-2441 | One-Part Optically Clear Epoxy Resin
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other
Main features
- High thermal stability (Tg = 157 °C)
- UV curable encapsulation
- High optical transmittance
Product Description
OPTOLINQ™ LE-2441 is a high-performance UV-curable epoxy resin developed for precision optical bonding and encapsulation. Engineered for fast and tack-free curing under 310–365 nm UV light, it offers superior optical clarity, strong adhesion, and robust thermal resistance. Its high refractive index (1.5665), >89% transmittance from 500 to 900 nm, and glass transition temperature of 157 °C make it ideal for LED optics, fiber-optic components, and sensor assemblies. LE-2441 is a solvent-free, single-component formulation with excellent flowability (viscosity: 2,500 ± 500 cP), and no pot life concerns. RoHS compliant and resistant to oxygen inhibition, it ensures stable processing and long-term performance in high-precision applications.
Product Key Features
- Fast UV curing – Cures quickly at 310–365 nm with minimal energy.
- Tack-free surface – Oxygen-insensitive curing avoids surface inhibition.
- High optical clarity – 90% transmittance at 900 nm; ideal for light-guiding applications.
- Optimal refractive index (1.5665), which is ideal for optical components.
- High Tg (157 °C) – Excellent thermal resistance for demanding environments.
- Low CTE (74 ppm/°C) – Ensures dimensional stability in optical assemblies.
- Strong adhesion to Si, Au, die attach materials, and printed circuit board assemblies, and forms airtight seals upon curing.
- Solvent-free, single-component – No mixing required; easy to handle and apply.
- RoHS compliant – Meets EU Directive 2011/65/EU for environmental safety.
Applications
- LED lens encapsulation and UV bonding
- Optical fiber and photonic component assembly
- Sensor and photodiode sealing
- Transparent coatings for display and imaging devices
- Precision bonding in optoelectronic modules
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Electrical Properties
Chemical Properties
Physical Properties
Additional Information
LE-2441 Recommended Curing Conditions
| Parameter | Value | Unit |
| Irradiation Wavelength | 310~365 | nm |
| Irradiation Intensity | 100 | mW/cm2 |
| Irradiation Energy Dose | 6000 | mW/cm2 |
Processing Instructions
- OPTOLINQ™ LE-2441 should be stored at 2–13 °C. Before use, keep the sealed container at ambient conditions for 1–2 hours. Do not open the lid until the temperature has equalised to prevent moisture condensation.
- Ensure that all application surfaces are clean, dry, and free of grease, dust, or mold-release agents. Wipe the surfaces with a suitable organic solvent to remove any contaminants that could affect the resin’s adhesion or curing performance.
- Avoid contact with substances that can inhibit curing, such as amines, amine-cured epoxies, or polyurethanes (PU). Direct or indirect exposure to these materials may reduce or completely prevent proper curing of LE-2441. It is recommended to perform compatibility testing prior to production use.
- Wear appropriate protective equipment and minimize direct contact with the human body. Refer to the Safety Data Sheet (SDS) before use.