OCA | optically clear adhesive film
Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls
Main features
- 91% Light transmittance
- 1 Optical haze
- Acid free
Product Description
LINQTAPE OCA is a film made out of Optically Clear Adhesive (OCA) backed on a PET substrate. OCA is a double-sided adhesive tape that is matrix-free, meaning it contains no supporting material.
LINQTAPE OCA has exceptional high visible light transmittance and low resistivity, making OCA film one of the most versatile and high-performance conductive materials available.
Applications include:
- Transparent device bonding: With exceptional light transmittance of up to 91%, our OCA Film guarantees crystal-clear visibility within the visible spectral region.
- Display assembly: With exceptional light transmittance of up to 91%, our OCA Film guarantees crystal-clear visibility within the visible spectral region.
- Areospace and militairy optic assembly: With exceptional light transmittance of up to 91%, our OCA Film guarantees crystal-clear visibility within the visible spectral region.
- Lenses: With exceptional light transmittance of up to 91%, our OCA Film guarantees crystal-clear visibility within the visible spectral region.
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Electrical Properties
Other Properties
Mechanical Properties
Additional Information
Key Optical and Physical Properties:
-
Optical Haze: <1
-
Light Transmittance: >91%
-
Physical Glue: >1500 g/25mm
-
Release Force of Light Release Film: <10 g/25mm
-
Release Force of Heavy Release Film: 25-30 g/25mm
Environmental Test Results:
- Hot and Humid (60°C, 90%RH, 240 Hours): PASS
- Thermal Shock (40°C~80°C, 30min/cycle, 200 Cycles): PASS
- High Temperature (80°C, 240 Hours): PASS
- Low Temperature (-40°C, 240 Hours): PASS
Key Features:
- Excellent optical performance: achieving transmittance of 92% or higher, with haze below 1.
- Acid-free: material with no corrosion impact on the adherend.
- Durability: Demonstrates durability without yellowing or bubble formation.
- Performance in variable conditions: Exhibits excellent performance under high and low-temperature conditions.
- Price die cutting: Ensures precise die-cutting with no overflow.