OCP-01 | Color Pigment pastes for Epoxy resins
Harmonization Code : 3205.00.00.90 | Colour lakes; preparations as specified in note 3 to this chapter based on colour lakes : Other
Main features
- Compatible with Epoxy resins
- Small amount needed
- Easy dispersion
Product Description
OCP-01 Color pigment pastes are transparent liquids, used as color additives for epoxy photoelectric resins. They are fully compatible with the epoxy resin chemistry and they require only a small amount on the total formulation weight (±0.1 - 0.5%).
OCP01-R, OCP01-G and OCP01-B pastes (Red, Green, Blue) have low viscosity and disperse very easily, making them cost effective due to their weight ratio. In addition to that they offer good anti-yellowing and good color fixing abilities.
Reference dosage:
· 0.1~0.5% of total epoxy resin formulation.
Packaging
Technical Specifications
No specifications available.
Additional Information
Instructions
- The product has been evenly dispersed and has good compatibility with epoxy resins. It can be directly added and used. In order to ensure the dispersion in the epoxy resin formulation, please stir it at high speed.
- This product is recommended to be stored in a cool, well-ventilated place.
- Please close the lid tightly after using to avoid moisture absorption.
- When this product is stored for a long time, there will be a slight layering phenomenon, which is normal. Stir the product before usage.
The above performance data is measured in a laboratory environment with a temperature of 25°C and a humidity of 70%. They are only used for reference and cannot guarantee what can be achieved in a particular environment.