OLS-1000 | Liquid Encapsulant - Two part Epoxy

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

White LED Cast OLS-1000 | Liquid Encapsulant - Two part Epoxy Optically Clear Two-Part Epoxy LED Liquid Encapsulant Photodiode Sensor IR LED Casting Sensor LED Color Casted Devices

Main features

  • Liquid epoxy encapsulant
  • Cost/Performance balance
  • Value engineered - Low cost

Product Description

OPTOLINQ OLS-1000 is a two-part (Part A & Part B), optically clear epoxy casting compound designed for the encapsulation of LED lamps and displays. It features excellent UV resistance, high optical transmittance, high adhesion to a range of substrates, and good thermal shock resistance. It is geared specifically for applications that will not be exposed to temperatures above 125°C, and where the cost of the encapsulation material is a large percentage of the final part cost. The OLS-1000 has been value-engineered to provide the minimum level of acceptable performance for the absolute lowest cost.

OPTOLINQ OLS-1000 has been used extensively for low-power LED encapsulation, automatic LED casting, and potting of large optoelectronic modules. Each of these applications relies on the high clarity and other optical properties of the OLS-1000 as well as its excellent mechanical properties. The OLS-1000 can be colored and diffused by the addition of specific dye concentrates and diffusant concentrates. This product is not made for SMD encapsulation but mainly for DIP packages. 

 
Newer Versions with improved optical and mechanical performance:
 
Product Family

LINQ OLS-1000

No longer available

This product is no longer available from Krayden. Please contact us so we can recommend an alternative product.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type Chemistry Type
Epoxy
Refractive index Refractive index
1.52
Specific Gravity Specific Gravity
1.16
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
130 °C
Temperature Resistance Temperature Resistance
125 ˚C
Electrical Properties
Volume Resistivity Volume Resistivity
100000000000000 Ohms⋅cm
Chemical Properties
Moisture absorption Moisture absorption
0.35 %

Additional Information

 

Additional Handling Instructions

Preheat Part A to 40°C and then mix in Part B in the required mixing ratio given above. Ideally, the mixture of Part A and B will be done in a vacuum and degassed at 3 torr (400 Pa) for 10-15 minutes. This will ensure that all the entrapped air bubbles are removed after mixing. For best results, ensure that all moisture has been removed from the parts to be encapsulated by preheating them for 1 hour @ 90°C. Also for best results, the encapsulation should be carried out in a vacuum.

Using Additives with OLS-1000

Optolinq OLS-1000 can be mixed with diffusing agents or color pastes to achieve customer-specific purposes.

Recommended quantity (in weight %) of various diffusing agents and color pastes to be used with OLS-1000:

  • OCP01-R Red Color Paste: 2-5% by weight
  • OCP01-B Blue Color Paste: 1-3% by weight
  • OCP01-G Green Color Paste: 2-4% by weight
  • ODF-10 Diffusing Agent: 2-5% by weight

Values with our latest pastes and agents TBD.

Storage and Handling

OPTOLINQ OLS-1000 is supplied in cans and jars and should be kept in a cool (10°C – 25°C) dry place (40% – 75% humidity) away from direct sunlight or temperature extremes. Part B is particularly sensitive to moisture, so be sure to remove moisture after using and to keep the lid of the container tightly sealed after use.

For safe handling information on this product, consult the Safety Data Sheet, (SDS).

The data contained herein may be reported as a typical value and/or range values based on actual test data and are verified on a periodic basis.

Leading Brands Trust in Our Products and Services