OLS-1000LV | Liquid encapsulant - Two part Epoxy
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other
Main features
- Extremely Low viscosity
- Rapid Cure
- Visible Light Blocking
Product Description
OPTOLINQ OLS-1000LV produces cured products with outstanding mechanical strength, excellent electrical performance, and superior high-temperature resistance. It is a reliable choice for high-quality surface mount LED packages requiring uniform light transmittance and visible light blocking. OLS-1000LV is available with visible light blockers with onset transmittances at 700, 750, and 835 nm.
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Electrical Properties
Chemical Properties
Physical Properties
Additional Information
OPTOLINQ OLS-1000 Series | Visible Light Blocking Capabilities
OLS-1000LV and OLS-1000HV are developed with compatibility to various dyes with different onset transmittance as shown.

Processing Instructions:
- Pre-heat Part A at 45~60°C for a maximum of 24 hours.
- Mix components A and B and stir uniformly.
- Defoam the mixture for 5 minutes.
- Curing conditions (Determine according to the specific needs of the product, following conditions are for reference only.)
Cure at 130 - 145°C/1 - 1.5hrs
Precautions:
- For optimal results, use the mixture within 6-8 hours after combining components A and B. Delaying application may lead to an undesirable increase in viscosity.
- Bake the molded package as soon as possible to prevent degradation by moisture.
- Pre-heating component A at 45~60°C can reduce viscosity, but excessively high temperatures will shorten the its pot life.
- Store the curing agent (component B) in sealed jars to prevent moisture absorption and sedimentation.
- Avoid skin and eye contact. In case of contact, rinse thoroughly with soap (for skin) or clean water (for eyes), and seek medical attention if needed.
- Maintain a clean and ventilated workplace, using extraction trunks when necessary.
- Wear appropriate protective equipment and minimize direct contact with the human body. Refer to the Safety Data Sheet (SDS) before use.
Please note that the provided information is based on available data and typical conditions. For specific applications and detailed test results, refer to the actual test data and conduct appropriate certifications.
Storage and Handling
Store in a ventilated, dry, and clean environment below 25°C. Keep away from fire and heat sources. It is strictly forbidden to store in outdoor environments. At proper storage conditions, Part A has a shelf life of 6 months and Part B a shelf life of 3 months. Shelf life can be extended by using cold storage.