PIT1A-WL-SG | 1-mil White Polyimide (Kapton) Tape with Acrylic Adhesive

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

PIT1A-WL-SG | 1-mil White Polyimide (Kapton) Tape with Acrylic Adhesive

Main features

  • 1 mil polyimide film
  • Acrylic adhesive
  • White-labeled

Product Description

LINQTAPE PIT1A-WL-Series is a Kapton Tape Alternative used for thermal printing. It provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures (-40 to 572 °F). It can be used in applications that require thermal printing on parts that can withstand high temperatures, such as steel or other alloys.

LINQTAPE™ PIT1A-WL-SG is a white top coated high-temperature resistant polyimide film, with a one-sided aggressive acrylic adhesive, and backed with a Kraft liner. The tape complies with RoHs and Reach requirements. 

 

Application Ideas

  • Label and bar code making 
  • Marking electronic components
  • Thermal printing
Product Family

LINQ PIT1A-WL-SG

1. Select Width
2. Select Length
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 6 weeks
CA Shipping in 6 weeks
EU Shipping in 6 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Temperature Resistance Temperature Resistance
300 ˚C
Electrical Properties
Breakdown Voltage Breakdown Voltage
6000 V
Other Properties
RoHS Compliant RoHS Compliant
Yes
Mechanical Properties
Adhesion Strength Adhesion Strength
25 Oz/in
Elongation Elongation
40 %
Tensile Strength (Thin Film) Tensile Strength (Thin Film)
52 N/cm
General Properties
Adhesive Thickness Adhesive Thickness
38.1 µm
Chemistry Type Chemistry Type
Polyimide
Color Color
White
Film Thickness Film Thickness
25.4 µm
Release Liner Release Liner
Kraft
Single or Double-Sided Adhesive Single or Double-Sided Adhesive
Single-Sided
Special Layer Special Layer
Thermal Ink Print Layer
Total Thickness Total Thickness
63.5 μm