Sn63Pb37 | Eutectic Solder Spheres
Harmonization Code : 8001.20 | Unwrought tin: Tin alloys
Main features
- Eutectic Solder Spheres
- Tin lead
- For BGA and CSP components
Product Description
LINQALLOY Sn63Pb37 Eutectic Solder Spheres are Tin-Lead eutectic solder spheres for BGA and CSP components used by companies who have not yet made the transition to Lead-free (Pb-free) soldering.
Each jar has a clear label on the lid specifying the solder ball diameter as well as a label on the front identifying the alloy type, the quantity of spheres in the jar, the date of manufacture, and the product lot (or batch) number. This batch number is also tied to a certificate of conformance that is also provided with the solder spheres and ensures the Sn63Pb37 solder spheres meet the following quality criteria:
- Tin (Sn): 63%
- Lead (Pb): 37%
- Melting Temperature (Eutectic): 183°C
- Sphericity : Within 1.5%
Diameter Tolerance
- 0.1mm - 0.25mm (100µm - 250µm) : ± 0.0050mm (± 5µm)
- 0.3mm - 0.45mm (300µm - 450µm) : ± 0.010mm (± 10µm)
- 0.5mm - 0.89mm (500µm - 890µm) : ± 0.020mm ( ± 20µm)
Typical Shelf life is 1 year. If Sealed we can guarantee an extension through CoC for one year from the purchase date instead of the mfg date.
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
What do I get when I buy Sn63Pb37 Solder Spheres from KRAYDEN?
The advantage of ordering solder spheres online at KRAYDEN.com is that you can be sure of the quality. The solder spheres you receive are originally manufactured solder spheres packed into jars with inert gas (nitrogen). We do not repack the solder balls we receive, so the jars you will receive have never been opened, thus ensuring the quality of the product you receive. The lid of the jar is also always sealed with a shrink-wrapped plastic wrap ensuring that the solder spheres do not oxidate in the jar.
| Description | Popular Brand1 Names |
|---|---|
| Tin/Lead (Sn63Pb37) Eutectic Solder Spheres. Products similar to LINQALLOY Sn63Pb37 Solder Spheres |
|
| 1 Sparkleballs®, Multicore Accurus®, Micrometal®, Precision Spheres®, Alphametal® and Ultra-Spheres® are registered trademarks of Senju, Henkel, NMC, Indium, Cookson and Kester respectively and are not affiliated with this site. | |