LINQSTAT VCF-3S100K is a black, carbon-filled, electrically conductive polyethylene plastic film designed to provide both physical and static protection. Having a surface resistance of 100,000 ohm-sq, (1x105 Ω-sq) it offers medium-level static protection which means it effectively avoids accumulation of electric charge on itself and the products which it protects. Its easy-grounding nature makes it ideal for packaging where electrostatic contamination is a problem. Keep in mind that the value is "below 100,000ohms-sq" and not an absolute number.
VCF-3S100K is useful in applications where the key is to balance cost versus performance. As a medium-level conductive plastic, the carbon-loading is such that it is low-enough to be cost-effective, while being high enough to meet the electrical requirements of military specification MIL-PRF-81705D Type II and MIL-P-82646A. It is typically used as an antistatic smartcard and micromodule interleaver.
VCF-3S100K film and its conductivity are unaffected by humidity and age. It gives good thermal stability and has outstanding chemical resistance. It has a standard thickness of 3mil(0.07mm) and is available in 35mm rolls, ideal for smartcard and micromodule interleaving applications.
Production batches from 2023 will have a Tolerance of ±50,000 ohms
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Electrical Properties
Other Properties
Additional Information
In sheet form, LINQSTAT VCF, works as an antistatic plastic. For more sensitive pressure sensor applications, KRAYDEN recommends LINQSTAT XVCF-Series, which is a more-conductive series of polyethylene plastics. As an antistatic packaging plastic, it is also used as a antistatic interleaver for Smartcard (micromodule) applications to separate subsequent layers of smartcard chips in micromodule production.
Product Applications
- Protection and storage of static-sensitive components
- Interleaf between rolls of Smartcard modules
- Grounding Mats
Product Features and Benefits
- Volume-conductive plastic
- Black Opaque - Printable
- Provides Anti-Static protection to electronics components
- Groundable
- Humidity independent conductivity
- Meets military specification MIL-P-82646A
Chemical Susceptibility
- Methanol: Resistant
- Ethanol: Resistant
- Isopropanol: Resistant
- Weak Acids: Resistant
- Ketones (Acetone): Slow Attack
- Weak Alkalines: Slow Attack
- Hydrocarbons: Non-Resistant