LINQBOND PM-2632 | Two part epoxy resin potting material
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other
Main features
- Low viscosity
- Low-temperature curing
- Ideal potting material for capacitors and epoxy resin for edge casting
Product Description
LINQBOND PM-2632 is a black, two-part flame-retardant potting epoxy resin. With its low viscosity after mixing, it offers a long service life and easy application process. PM-2632 can be cured at low temperature, and once cured, it exhibits excellent electrical, thermal dissipation, and mechanical properties.
LINQBOND PM-2632 is an ideal potting material for small electronic components, such as capacitors, and epoxy resin for edge casting applications. Its operating temperature is -20 up to 100°C.
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Electrical Properties
Additional Information
Premixed Properties
|
Property |
Part A |
Part B |
|
Appearance |
Black liquid |
Light yellow transparent liquid |
|
Specific gravity at 25 °C |
1.55±0.05 |
1.09±0.01 |
|
Viscosity at 25 °C |
9700±2300 cP |
100±20 cP |
|
Shelf life |
183 days |
183 days |
Precautions for Use
- Storing Part A for an extended duration may cause filler precipitation. Stir thoroughly before use to achieve uniform filler distribution.
- During cold seasons, preheat Part A at 30–50 °C for best results.
- The usable time of Parts A and B after mixing is affected by temperature and mixing volume. The higher the temperature and the larger the mixing volume, the shorter the usable time. Therefore, the mixing temperature and mixing volume should be determined according to the on-site operation.
- Please wear relevant protective equipment before use, minimizing direct contact with the skin. Pay careful attention to the details and review the Material Safety Data Sheet (SDS) before initiating use.
Storage and Handling
Store in a ventilated, dry, and clean environment at room temperature. Keep away from fire and heat sources. At proper storage conditions, Part A and Part B both have a shelf life of 183 days. Shelf life can be extended by using cold storage.