LINQBOND UF3802 | Reworkable BGA & CSP Underfill
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other
Main features
- High Tg
- Very low viscosity
- One-component
Product Description
Cure Schedule
- 130°C for 30 min
- Alternative Cure schedule:
- 150°C for 5 - 8 min
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Physical Properties
Additional Information
Instructions for Use:
-
Before use, thaw the product to reach room temperature for 1–2 hours. The syringe should be placed vertically while thawing. Keep the container airtight until room temperature is reached.
-
Ensure the surface to be bonded is clean and free of contaminants like dirt, grease, or mold release agents. A simple solvent wipe is often sufficient.
-
Cure time may vary based on the actual part geometry, material volume, and equipment. It is recommended that the test be done on actual parts and equipment.
-
For large-scale applications, consider a staged curing process: start with a lower temperature pre-cure, followed by a full cure at a higher temperature to manage heat release effectively.
-
Cool down gradually after curing to minimize thermal stress.
-
The epoxy cannot be refrozen once exposed to room temperature.
Rework Process:
-
Component Removal. Component solder joints must be heated above their reflow temperature (260°C to 280°C). At this temperature, the undefill will be soft and easy to remove. Component may then be pulled or removed by twisting or with a use of a vacuum pick-up nozzle.
-
Site Preparation. After component removal, cleaning of residues may be done by the following methods
-
Scraping. Heat the site to 250°C to 300°C and scrape off the underfill carefully avoiding damage of pads on the substrate. Alternatively, heating can also be done from the bottom of the substrate.
-
Rotating Brush. Apply sufficient amount of pressure onto the brush to clean the residues. Care should be taken to avoid damage to substrate.
- Component Replacement. Isopropanol or a flux pen may be used to ensure no residue remains on the circuit board after cleaning. Brush solder paste or flux on the board and align the new component using a vacuum and reflow using hot air. Underfill will likewise be applied followed by cure step.
Storage and Handling
Store and transport below -5°C temperature. Keep away from moisture and heat sources. It is strictly forbidden to store in outdoor environments.