LINQCELL GDL2900 | 2.9mm Carbon Plate
Harmonization Code : 6815.11.00.00 | Articles of stone or of other mineral substances, not elsewhere specified or included; Non-electrical articles of graphite or other carbon; Carbon fibres and articles of carbon fibres
Main features
- 2.9mm - 2900um - 114mil
- Thickest GDL available
- Graphitized Carbon Plate
Product Description
LINQCELL GDL2900 is a graphitized carbon plate, commonly used as a gas diffusion layer and electrode for fuel cells. Its through plane resistance is less than 25 mΩcm2. It has a thickess of 2.9mm that is measured at 50 kpa.
LINQCELL GDL2900 has a density of ±0.60 g/cm3 and a through plane resistivity of 90mΩ-cm instead of 100mΩ-cm from the classic Spectracarb grades. Voltage loss is 28mV. Shortly, we should be able to die cut circles and most designs that you might require.