LINQCELL GDP340 | 340um Non woven Carbon Paper
Harmonization Code : 6815.11.00.00 | Articles of stone or of other mineral substances, not elsewhere specified or included; Non-electrical articles of graphite or other carbon; Carbon fibres and articles of carbon fibres
Main features
- 0.34mm - 340um - 13.4mil
- Non woven
- Highly flexible - Roll form
Product Description
LINQCELL GDP340 is a non woven carbon paper with a Microporous layer and PTFE. It is commonly used as a gas diffusion layer and electrode for fuel cells. Its through-plane resistivity is less than 10 mΩcm2. The thickness can reach 0.18mm at 1mPa. This carbon paper is highly flexible and has excellent air permability.
LINQCELL GDP340 is a close alternative to the discontinued Spectracarb 1550. This gas diffusion layer can be compressed ~50% at 100kPa. It is the only product that comes in long roll form.