LOCTITE 087
Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other
Main features
- High-Strength Coarse-Thread Retention
- 11.3 to 28.3 N m Prevail Torque
- One-Part Heat-Assisted Disassembly
Product Description
LOCTITE GRD AV High-Strength Threadlocker is a one-part red anaerobic liquid for locking and sealing large, coarse-threaded nuts, bolts, and studs. Its 100 to 250 mPa s viscosity supports controlled application before assembly, and the high-strength cured bond is intended for fasteners requiring durable retention. After 24 hours at 22 deg C, it develops 7 N m breakaway torque and 11.3 to 28.3 N m prevail torque on 3/8 x 24 grade 2 steel fasteners under ISO 10964 testing. The product requires no mixing; disassembly is performed with localized heat when removal is necessary. Applications include large coarse-threaded metal assemblies where high locking strength is required.
Key features
- High-Strength Coarse-Thread Locking: The red anaerobic liquid is intended for large coarse-threaded fasteners requiring high locking strength.
- 11.3 to 28.3 N m Prevail Torque: Typical prevail torque is measured after 24 hours at 22 deg C on grade 2 steel fasteners.
- Heat-Assisted Disassembly: Localized heat enables removal when the high-strength threaded assembly must be disassembled.
Applications / Suitable for
- Large coarse-threaded nuts, bolts, and studs
- High-strength metal fastener retention
- Threaded assemblies requiring locking and sealing
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Thermal Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Typical uncured and storage properties for LOCTITE GRD AV.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Red liquid | Uncured material; LMS | |
| Components | One | component | No mixing required |
| Viscosity | 100 to 250 | mPa s | Cannon-Fenske; ISO 3104; uncured material |
| Specific gravity | 1.07 | At 25 deg C; uncured material | |
| Cure mechanism | Anaerobic | Threadlocking application | |
| Optimal storage | 8 to 21 | deg C | Unopened container in a dry location |
After-processing / final-state properties
Typical cured-material and threaded-fastener results for LOCTITE GRD AV.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Breakaway torque | 7 | N m | After 24 hours at 22 deg C; ISO 10964; 3/8 x 24 grade 2 steel nuts and bolts |
| Prevail torque | 11.3 to 28.3 | N m | After 24 hours at 22 deg C; ISO 10964; 3/8 x 24 grade 2 steel nuts and bolts |
| Dielectric breakdown strength | 9.8 | kV/mm | IEC 60243-1; cured material |
| Thermal conductivity | 0.1 | W/(m K) | ISO 8302; cured material |
| Coefficient of thermal expansion | 100 x 10^-6 | K^-1 | ISO 11359-2; cured material |
| Specific heat | 0.3 | kJ/(kg K) | Cured material |