LOCTITE 545

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 545

Main features

  • One-Component Sealing System
  • Thread Sealing and Locking
  • Assembly Lubricity Sealant Formulation

Product Description

LOCTITE® 545 is a single-component, medium-viscosity anaerobic thread sealant designed for locking and sealing close-fitting metal pipes and fittings. The purple methacrylate ester formulation cures when confined between metal surfaces in the absence of air, helping prevent loosening and leakage caused by shock and vibration. It is specially formulated to provide lubricity during assembly and is suitable for hydraulic and pneumatic threaded connections.

Key features

  • Thread sealing and locking: Helps prevent leakage and loosening in close-fitting metal threaded assemblies.
  • Assembly lubricity: Formulated to support easier assembly of metal pipes and fittings.
  • One-component anaerobic cure: Requires no mixing and cures when confined between mating metal surfaces.
Product Family

LOCTITE 545

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance Appearance
Purple liquid
Specific Gravity Specific Gravity
1.02
Physical Properties
Viscosity Viscosity
9,000 - 20,000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured material; values are reference data rather than guaranteed product specifications.

Property Value Unit Method / condition
Technology Acrylic — Uncured material
Chemical type Methacrylate ester — Uncured material
Appearance Purple liquid — Uncured material
Components One component — No mixing required
Viscosity 9,000–20,000 mPa·s Brookfield RVT, 25°C; spindle 3, 2.5 rpm
Specific gravity 1.02 — At 25°C
Flash point >93 °C Tagliabue closed cup; SDS value
Technical properties

After-processing / final-state properties

Typical cured-material properties depend on the stated cure schedule, substrate, specimen, and test method.

Property Value Unit Method / condition
Coefficient of thermal expansion 80 × 10−6 K−1 ISO 11359-2
Thermal conductivity 0.1 W/(m·K) ISO 8302
Specific heat 0.3 kJ/(kg·K) Typical cured-material property
Breakaway torque 2 N·m ISO 10964; M10 steel nuts and bolts; cured 24 hours at 22°C
Compressive shear strength ≥1.5 N/mm² ISO 10123; steel pins and collars; cured 24 hours at 22°C
Cold-strength test limit −75 °C Product tested to this temperature

Leading Brands Trust in Our Products and Services