LOCTITE SF 713 is a transparent, colorless to slightly amber, very-low-viscosity cyanoacrylate activator for pre- or post-application cure acceleration. The amine active ingredient is supplied in isopropanol and dries in 30 seconds or less at 20 deg C. Its short on-part life of one minute or less supports rapid, controlled assembly sequences rather than long staging intervals. The activator is used with compatible cyanoacrylate adhesives to secure wires or coils to printed circuit boards, tamperproof adjustable components, and mount stand-offs, edge guides, or board stiffeners.
Key features
- Pre- or post-application use: The activator can be applied before adhesive placement or to exposed adhesive afterward.
- Rapid 30-second drying: The isopropanol carrier dries in 30 seconds or less at 20 deg C.
- Short controlled process window: On-part activity lasts one minute or less under the listed condition.
Applications / Suitable for
- Securing wires and coils to printed circuit boards
- Tamperproofing adjustable components
- Mounting stand-offs, edge guides, and board stiffeners
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Physical Properties
General Properties
Additional Information
As-supplied / before-processing properties
Typical values and characteristics for the product before cure, application, or assembly.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Transparent, colorless to slightly amber liquid | - | As supplied |
| Active ingredient | Amine | - | 1.7% to 2.3% |
| Solvent | Isopropanol | - | Carrier |
| Specific gravity | 0.8 | - | 25 deg C |
| Viscosity | 1 | mPa s | 20 deg C |
| Drying time | <=30 | s | 20 deg C |
| On-part life | <=1 | min | After application |