Loctite 9696.060NW AERO

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite 9696.060NW AERO

Main features

  • Metal-to-Aluminum Epoxy Bonding
  • 225 to 265 deg F Cure Window
  • 250 deg F Service Temperature

Product Description

LOCTITE EA 9696 AERO Epoxy Film Adhesive is a modified epoxy film adhesive for metal-to-metal and honeycomb bonding. It combines high toughness with a defined service temperature of 250°F (121°C), based on retaining 1,000 psi (6.9 MPa) tensile lap shear strength under ASTM D1002 testing. The film supports cure temperatures from 225°F to 265°F (107°C to 129°C) and provides balanced flow for both bonding configurations. Long room-temperature out-time supports production-floor and repair handling, while documented strength retention after hot/wet, fuel, hydraulic-fluid, de-icing-fluid, and dry-heat conditioning supports evaluation for environmentally demanding bonded assemblies.

Key features

  • Metal and honeycomb bonding: Balanced-flow film is suitable for metal-to-metal and aluminum-honeycomb bonding applications.
  • Flexible thermal cure window: Supports cure for 60 to 90 minutes between 225°F and 265°F (107°C and 129°C).
  • Extended shop out-time: May be used for at least 60 days at 77°F (25°C) or 30 days at 90°F (32°C) after removal from refrigerated storage.

Applications / Suitable for

  • Metal-to-metal bonding
  • Aluminum-honeycomb bonding
  • Shop-floor and repair bonding operations requiring extended out-time
  • Sound-suppression assemblies using reticulated adhesive film
Product Family

LOCTITE 9696 AERO

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Storage and handling characteristics for the epoxy adhesive film before cure.

Property Value Method / condition
Product form Modified epoxy adhesive film As supplied
Recommended storage temperature 0°F (-18°C) or below Store in sealed containers to prevent moisture contamination
Warranty storage life 12 months from date of shipment Stored at 0°F (-18°C)
Open assembly time At least 60 days at 77°F (25°C); at least 30 days at 90°F (32°C) After removal from refrigerated storage
Technical properties

After-processing / final-state properties

Typical cured bulk-resin and bonded-joint properties. Performance depends on film construction, cure schedule, substrate preparation, and test configuration.

Property Typical value Method / condition
Service temperature 250°F (121°C) Temperature at which the adhesive retains 1,000 psi (6.9 MPa), ASTM D1002
Glass transition temperature, dry 253°F (123°C) DMTA, E′ curve
Glass transition temperature, wet 200°F (93°C) DMTA, E′ curve; conditioned at 160°F (71°C) and 98% RH to moisture equilibrium
Cured density 1.14 g/mL Bulk resin
Moisture uptake <3% Wet conditioning at 160°F (71°C) and 98% RH to moisture equilibrium
Ultimate tensile strength at 77°F (25°C) 6,839 psi (47.2 MPa) 0.125 in (3.18 mm) casting, ASTM D638; cured 60 minutes at 250°F (121°C)