LOCTITE AA 3103
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- UV/Visible-Light Adhesive Cure
- High-Adhesion Adhesive Bonding
- Polycarbonate Bonding Application
Product Description
LOCTITE® AA 3103™ is a one-component UV and visible light-curing acrylic adhesive specifically formulated for bonding polycarbonate components while minimizing the risk of stress cracking under typical molded stress conditions. The transparent, flexible adhesive cures rapidly upon exposure to suitable ultraviolet or visible light sources, enabling high-speed production processes. LOCTITE AA 3103 develops strong, transparent bonds with a wide variety of substrates including polycarbonate, glass, many plastics and most metals. Its thixotropic consistency reduces adhesive migration after application, allowing precise placement and improved bond-line control.
Key Features & Benefits
- UV and visible light-curing adhesive for rapid processing.
- Specially designed for bonding polycarbonate without stress cracking.
- Forms flexible, transparent bonds.
- Excellent adhesion to glass, plastics and metals.
- Thixotropic formulation minimizes adhesive migration.
- One-component system requiring no mixing.
- Enhances load-bearing and shock-absorbing characteristics of bonded assemblies.
Recommended Applications
- Polycarbonate-to-polycarbonate bonding.
- Transparent plastic assembly applications.
- Glass-to-plastic bonding.
- Medical, electronic and industrial component assembly.
- High-speed production environments utilizing UV curing systems.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
As-Supplied / Before-Processing Properties
| Property | Value | Unit | Condition |
|---|---|---|---|
| Technology | Acrylic | — | UV / Visible Light Cure |
| Chemical Type | Acrylated Urethane | — | One-component adhesive |
| Appearance | Transparent to Slightly Hazy | — | Liquid |
| Viscosity Classification | Medium, Thixotropic | — | Uncured material |
| Specific Gravity | 1.13 | — | 25°C |
| Refractive Index | 1.48 | — | Uncured |
| Brookfield Viscosity | 8,000 - 14,500 | mPa·s | RVT, spindle 5, 20 rpm, 25°C |
| Fixture Time | ≤18 | seconds | UV cure, glass microscope slides |
After-Processing / Final-State Properties
| Property | Value | Unit | Condition / Method |
|---|---|---|---|
| Shore Hardness | 51 | Shore D | ISO 868 |
| Refractive Index | 1.50 | — | Cured adhesive |
| Elongation at Break | 260 | % | ISO 527-3 |
| Tensile Strength at Break | 17 | N/mm² | ISO 527-3 |
| Tensile Modulus | 207 | N/mm² | ISO 527-3 |
| Lap Shear Strength | 11 | N/mm² | ISO 4587, polycarbonate |
| Surface Resistivity | 8.7 × 10¹⁴ | Ω | IEC 60093 |
| Volume Resistivity | 8.9 × 10¹⁴ | Ω·cm | IEC 60093 |
| Dielectric Breakdown Strength | 24 | kV/mm | IEC 60243-1 |