LOCTITE CAT 21

Main features

  • Low-Viscosity Polyoxyalkylene Amine Curative
  • One-Hour Pot Life
  • Large-Mass Epoxy Castings

Product Description

LOCTITE® CAT 21 is a low-viscosity polyoxyalkylene amine curing agent designed for use with compatible epoxy resin systems. The hardener is particularly suited for large-mass casting applications and provides excellent impact resistance, thermal shock resistance and non-crystallizing storage stability. It can be cured at room temperature or with elevated-temperature post-curing and delivers reliable performance in epoxy systems operating across a broad temperature range.

Key Features & Benefits

  • Polyoxyalkylene amine epoxy curing agent.
  • Low-viscosity formulation for easy processing.
  • Non-crystallizing during storage.
  • Suitable for large-mass epoxy castings.
  • Good impact resistance after cure.
  • Good thermal shock resistance.
  • Supports room-temperature and heat-cure schedules.

Recommended Applications

  • Large-volume epoxy casting systems.
  • Industrial encapsulation and potting.
  • Electrical and electronic resin systems.
  • Applications requiring thermal shock resistance.
  • General-purpose epoxy curing applications.
Product Family

LOCTITE CAT 21

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Polyoxyalkylene Amine — Epoxy Curing Agent
Appearance Dark Amber — As supplied
Viscosity 65 mPa·s (cP) 25°C
Specific Gravity 1.03 — 25°C
Pot Life (100 g Mass) 1 hour 25°C
Shelf Life 548 days 25°C storage
Cure Type Room Temperature or Heat Cure — Recommended process
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Recommended Cure Schedule 16 - 24 hours 25°C initial cure
Post Cure 6 hours 65 to 85°C
Continuous Operating Temperature -65 to +120 °C Typical cured epoxy system
Impact Resistance Good — Product characteristic
Thermal Shock Resistance Good — Product characteristic
Large Mass Casting Capability Yes — Designed for large epoxy castings
Crystallization Resistance Non-Crystallizing — Storage characteristic