Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE E-04

Main features

  • Two-Component Adhesive System
  • Thixotropic Application Control
  • Low-Shrinkage Epoxy Bonding

Product Description

LOCTITE® E-04 is a two-component toughened epoxy adhesive designed for structural bonding of metals, magnets, glass and engineering plastics. The adhesive cures at room temperature to form a durable, impact-resistant bond with excellent electrical insulation properties, low shrinkage and good chemical resistance. Its thixotropic consistency and gap-filling capability make it suitable for demanding industrial assembly and repair applications.

Key Features & Benefits

  • Two-component toughened epoxy technology.
  • Thixotropic, non-flowing adhesive consistency.
  • Low shrinkage during cure.
  • Excellent impact resistance.
  • Outstanding electrical insulation properties.
  • Good chemical resistance after cure.
  • Structural bonding of metals, magnets, glass and plastics.

Recommended Applications

  • Structural metal bonding.
  • Magnet assembly and ferrite bonding.
  • Glass bonding applications.
  • Plastic component assembly.
  • General industrial repair and maintenance.
Product Family

LOCTITE E-04

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Toughened Epoxy — Two-component adhesive
Appearance (Resin) White — Paste
Appearance (Hardener) Black — Paste
Appearance (Mixed) Gray — Mixed adhesive
Mixed Viscosity 77,500 cP 25°C
Specific Gravity 1.34 — Mixed, 25°C
Mix Ratio 1 : 1 Resin : Hardener By weight or volume
Work Life 45 minutes 25°C
Maximum Gap Fill 5.0 mm Typical value
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Full Cure Time 24 hours 25°C
Hardness 60 Shore D 25°C
Lap Shear Strength (Steel) 17 - 21 N/mm² ASTM D1002
Lap Shear Strength (Aluminum) 17 - 19 N/mm² ASTM D1002
Lap Shear Strength (Stainless Steel) 17 - 23 N/mm² ASTM D1002
Operating Temperature Range -55 to +70 °C Continuous service
Dielectric Strength 120 - 180 kV/cm Typical cured material
Dielectric Constant 3.5 - 6.0 — Typical cured material
Volume Resistivity >1 × 10¹⁴ Ω·cm Typical cured material