LOCTITE EA 11C
Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated
Main features
- Machinable, Low-Outgassing Cured Material
- Bonds Metals, Most Plastics and Wood
- Room-Temperature or Heat Cure
Product Description
LOCTITE EA 11C is a black, two-part epoxy adhesive and sealant for general-purpose bonding, sealing, and repair of metals, most plastics, and wood. The resin and hardener mix at 100:38 by weight or 2.5:1 by volume and provide at least 20 minutes of pot life at 25 °C. The system cures at room temperature or with heat, reaches handling strength in approximately 3 to 4 hours at 25 °C, and develops full cure after 72 hours at 25 °C. Once cured, the material can be machined and sanded and has documented high-service-temperature and low-outgassing characteristics.
Key features
- Multi-material bonding and repair for metals, most plastics, and wood.
- Room-temperature or heat cure with at least 20 minutes of pot life at 25 °C.
- Machinable, low-outgassing cured material with documented high-service-temperature capability.
Applications / Suitable for
- General-purpose bonding, sealing, and repair of metals, most plastics, and wood.