LOCTITE EA 9658.100

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LOCTITE EA 9658.100

Main features

  • Non-Woven Glass Film Support
  • 177 deg C High-Temperature Cure
  • Extended 15-Day Assembly Window

Product Description

LOCTITE EA 9658.100 PSF NWG AERO is the 0.100 lb/sf non-woven glass-supported configuration of a high-temperature epoxy film adhesive for nacelle metal, composite and honeycomb bonding. The film cures for 1 hour at 177 deg C and provides at least 15 days of open assembly time at 25 deg C or 10 days at 32 deg C. Its non-woven glass carrier supports the specified film construction, while controlled flow helps limit hole blockage and excess flash. Refrigerated storage at -18 deg C or below provides a 9-month warranty life.

Key features

  • Non-woven glass support: The 0.100 lb/sf NWG configuration uses a non-woven glass fabric carrier.
  • High-temperature cure: The film cures for 1 hour at 177 deg C under maintained pressure.
  • Extended assembly window: Open assembly time is at least 15 days at 25 deg C or 10 days at 32 deg C.

Applications

Applications include high-temperature nacelle metal, composite and honeycomb bonding where the 0.100 lb/sf NWG configuration is specified.

Product Family

LOCTITE EA 9658.100

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied properties

Configuration-specific and common EA 9658 handling values.

Property Value Unit Method / condition
ConfigurationEA 9658 .100 PSF NWGSpecific product variant
ConstructionNon-woven glass supportedNWG film
Standard package36 in x 150 ft450 sf roll
Open assembly timeAt least 15daysAt 25 deg C
Open assembly timeAt least 10daysAt 32 deg C
Storage temperature-18 or belowdeg CSealed container
Warranty life9monthsAt -18 deg C or below, from shipment
Cure schedule1 hour at 177 deg CHeat-up rate 2.2 to 4 deg C/minute

Leading Brands Trust in Our Products and Services