LOCTITE EA 9690.060K
Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics
Main features
- High-Peel Structural Bonding
- Knit-Supported Film Handling
- Sub-121 deg C Cure
Product Description
LOCTITE EA 9690.060K AERO is a 0.060 lb/sf knit-supported modified epoxy film adhesive for aerospace structural bonding. The low-flow film is formulated for metal, composite and honeycomb assemblies that require bond toughness and high peel capability. Its knit carrier supports handling of the specified film construction, and the adhesive cures below 121 deg C. The 36 in by 167 ft roll format supports lay-up in structural panels and sandwich constructions where the .060K grade is specified.
Key features
- High-peel structural bonding: The modified epoxy system is formulated for tough structural bonds with high peel capability.
- Knit-supported construction: The 0.060 lb/sf film uses a knit carrier for the specified .060K configuration.
- Lower-temperature cure: The film cures below 121 deg C.
Applications
Applications include aerospace metal, composite and honeycomb structural bonding where the .060K knit-supported configuration is specified.
TDS, SDS & Technical Documents
Technical Specifications
Thermal Properties
Additional Information
As-supplied properties
Physical format and supplied configuration.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Configuration | EA 9690 .060K | Specific product variant | |
| Film weight | 0.060 | lb/sf | Supplied film |
| Support carrier | Knitted | K configuration | |
| Roll width | 36 | in | Standard roll |
| Roll length | 167 | ft | Standard roll |
| Roll area | 501 | sf | Per roll |