LOCTITE ECI 1014 E&C
Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category
Main features
- Low temperature drying
- High conductivity
- Compatible for use with polycarbonate, polyester and polyurethane
Product Description
LOCTITE® ECI 1014 is a highly conductive, silver, high-elongation ink based on a thermoplastic polyurethane binder. This combined stretchability and high conductivity enables the development of medical wearables, smart textiles, automotive interiors, and flexible heater applications.
LOCTITE® ECI 1014 can be dried at temperatures as low as 80°C (176°F). It is suitable for screen printing or high-speed printing after dilution, and compatible with solvent-sensitive substrates such as polycarbonate, polyester or thermoplastic polyurethane.
Drying cycle
- 15 minutes @ 120°C
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
DIRECTIONS FOR USE
1. Surface Preparation
- Clean the surface thoroughly prior to application
2. Mixing/Dilution
- Mix thoroughly before use to ensure it is homogenous.
- Moderate heating of the ink, up to 40°C, can improve product homogeneity
- Should dilution be necessary use Dowanol DPM (CAS: 34590-94-8). Henkel recommends a maximum of 10 wt%. This should be accomplished by adding solvent at 0.5 wt% intervals by weight until desired viscosity and printability are achieved.
3. Application
- LOCTITE ECI 1014 E&C may be applied by screen printing method.
- Recommended screen and printing parameters are:
Emulsion Thickness, µm:
Solvent resistant 10 to 40
Squeegee Hardness 70 to 90
Screen Type, Polyester screen, cm 77-48