LOCTITE MR5412
Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.
Main features
- Solvent-Based Neoprene Contact Adhesive
- Fast Air-Dry Tack
- Repositionable During Initial Assembly
Product Description
LOCTITE® MR 5412 is a solvent-based neoprene rubber contact adhesive designed for maintenance, repair, and general-purpose bonding applications. The adhesive develops fast, high-strength bonds and provides waterproof performance on both porous and non-porous substrates. It is particularly suitable for bonding weatherstripping, insulation, rubber components, and trim materials to wood and metal surfaces, while allowing repositioning during assembly before final bond formation.
Key Features & Benefits
- Solvent-based neoprene rubber contact adhesive.
- Fast, high-strength bond development.
- Waterproof bond performance.
- Repositionable during initial assembly.
- Suitable for porous and non-porous substrates.
- Air-dry curing system.
- Strength increases with aging and moderate heat exposure.
Recommended Applications
- Weatherstripping installation and repair.
- Insulation bonding.
- Rubber-to-metal bonding.
- Trim attachment applications.
- Wood-to-rubber and wood-to-metal bonding.
- General maintenance and repair bonding.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Appearance
Appearance
Yellow liquid
Specific Gravity
Specific Gravity
0.88
Physical Properties
Viscosity
Viscosity
6,000 - 10,000 mPa.s
Additional Information
Technical Properties
As-Supplied / Before-Processing Properties
| Property | Value | Unit | Condition |
|---|---|---|---|
| Technology | Solvent Based Contact Adhesive | — | Neoprene rubber formulation |
| Chemical Type | Neoprene Rubber | — | Contact cement chemistry |
| Appearance | Yellow Liquid | — | As supplied |
| Specific Gravity | 0.88 | — | 25°C |
| Viscosity | 6,000 - 10,000 | mPa·s (cP) | Brookfield RV, 25°C |
| Solids Content | 30 - 34 | % | Non-volatile content |
| Weight per Gallon | 7.01 - 8.56 | lb/gal | Typical |
| Cure Mechanism | Air Dry | — | Solvent evaporation |
Technical Properties
After-Processing / Final-State Properties
| Property | Value | Unit | Condition / Benefit |
|---|---|---|---|
| Open Time Before Assembly | 3 - 4 | minutes | Allow adhesive to become tacky |
| Initial Bond Strength | High | — | Holds most assemblies immediately |
| Final Bond Strength | Maximum After Full Drying | — | Strength develops as solvent evaporates |
| Water Resistance | Waterproof | — | Suitable for weatherstrip applications |
| Repositionability | Yes | — | Allows adjustment during assembly |
| Porous Surface Compatibility | Suitable | — | Wood, insulation and similar materials |
| Non-Porous Surface Compatibility | Suitable | — | Metal and rubber bonding |
| Heat Aging Performance | Improved Strength | — | Moderate heat exposure increases bond strength |