LOCTITE SF7070
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Low-Viscosity Precision Cleaning
- 5-20 Minute Drying Window
- Spray, Wipe, or Immersion Use
Product Description
LOCTITE SF 7070 Cleaner and Degreaser is a one-part, non-aqueous hydrocarbon and monoterpene solvent cleaner for final pre-assembly surface preparation. The colorless, very-low-viscosity liquid removes greases, oils, lubricating fluids, metal cuttings, and fines before bonding with LOCTITE adhesives. It can be applied by spray, wipe, or immersion at room temperature or with controlled heating. The cleaner typically dries in 5 to 20 minutes at 20 deg C and does not change adhesive cure speed or final strength beyond providing a clean bonding surface.
Key features
- Low-viscosity surface cleaning: A 1 to 2 mPa s liquid reaches detailed surfaces for spray, wipe, or immersion cleaning.
- Pre-bond contaminant removal: Removes oils, greases, lubricating fluids, metal cuttings, and fines before adhesive assembly.
- Controlled drying window: Typically evaporates in 5 to 20 minutes at 20 deg C before bonding.
Applications
Applications include final pre-assembly cleaning and degreasing by spray, wipe, or immersion before bonding.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
As-supplied properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Colorless transparent liquid | As supplied | |
| Specific gravity | 0.75 | 25 deg C | |
| Viscosity | 1 to 2 | mPa s (cP) | 20 deg C |
| Kauri-butanol value | 31 | Typical property |