LOCTITE TC8M
Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses
Main features
- High Thermal-Conductivity Silicone Grease
- Electrical-Insulation Thermal Grease
- Corrosion-Protective Thermal Grease
Product Description
LOCTITE® TC 8M is a silicone-based thermal grease formulated for efficient heat transfer between heat-generating electronic components and heat-dissipating structures. The material combines high thermal conductivity with excellent electrical insulation and dielectric properties, making it suitable for a broad range of thermal management applications. It retains its paste-like consistency during prolonged exposure to elevated temperatures and is designed for use in semiconductor devices, thermoelectric equipment, radiators, power resistors, and chassis-mounted components. Based on the uploaded datasheet image.
Key Features & Benefits
- High thermal conductivity for efficient heat dissipation.
- Excellent electrical insulation properties.
- High dielectric strength.
- Maintains paste consistency at elevated temperatures.
- Suitable for thermal interface applications.
- Provides corrosion protection on mating surfaces.
- Easy application using syringes, cartridges, and dispensing equipment.
Recommended Applications
- Heat sinks in semiconductor devices.
- Thermostats in thermoelectric devices.
- Radiators and mounting surfaces.
- Power resistors.
- Electronic chassis assemblies.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
As-Supplied / Before-Processing Properties
| Property | Value | Unit | Condition |
|---|---|---|---|
| Technology | Silicone Grease | — | Thermal management compound |
| Appearance | White | — | As supplied |
| Viscosity | 1,300 | mPa·s (cP) | 25°C, 0.5 rpm |
| Viscosity | 330 | mPa·s (cP) | 25°C, 5 rpm |
| Density | 2.5 | g/cm³ | Typical value |
| Fineness | <50 | µm | Typical value |
| Shelf Life | 365 | days | 18 to 25°C storage |
| Operating Temperature Range | -40 to +200 | °C | Continuous operation |
After-Processing / Final-State Properties
| Property | Value | Unit | Condition / Method |
|---|---|---|---|
| Thermal Conductivity | 1.5 | W/(m·K) | Physical property |
| Weight Loss | 0.2 | % | 24 h @ 100°C |
| Dielectric Strength | 19 | kV/mm | Electrical property |
| Volume Resistivity | 1 × 10¹⁴ | Ω·cm | Electrical property |
| Thermal Management Performance | High | — | Enhances heat transfer between components |
| Electrical Insulation | High | — | High dielectric and resistivity properties |
| High Temperature Stability | Excellent | — | Retains paste consistency after heat exposure |