LORD 459X
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- Adhesion-Promoting Surface Treatment
- Low-Viscosity Adhesive Application
- Brush, Dip or Spray Application
Product Description
LORD® 459X Adhesion Enhancer/Surface Modifier is a low-viscosity, xylene-based surface treatment designed to promote adhesion to difficult-to-bond thermoplastic elastomers, thermoplastic polyolefins and EPDM. Supplied pre-diluted for direct application, it can be used with LORD acrylic, urethane and epoxy structural adhesives, as well as compatible coatings and double-sided tapes. The material requires no mixing or additional dilution and can be applied by brush, dip or spray.
Key Features
- Promotes adhesion to difficult elastomers, including TPE, TPO and EPDM substrates.
- Ready-to-use formulation requires no mixing or dilution before application.
- Low-viscosity application supports brush, dip and spray methods.
- Low dry-film requirement with an optimum dry-film thickness of approximately 0.1 mil (2.5 µm).
Applications / Suitable for
- Surface treatment of TPE, TPO and EPDM
- Adhesion promotion for acrylic, urethane and epoxy structural adhesives
- Adhesion enhancement for coatings
- Surface preparation for compatible double-sided tapes
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Thermal Properties
Additional Information
As-Supplied / Before-Processing Properties
Typical as-supplied properties. Values are typical and are not intended for specification purposes.
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Appearance | Amber liquid | — | Typical |
| Viscosity | Approximately 10 | cP | Brookfield LVT, Spindle 1, 60 rpm at 77°F (25°C) |
| Density | 7.15–7.35 (857–881) |
lb/gal (kg/m³) |
Typical |
| Solids Content by Weight | 2.7–4.1 | % | Typical |
| Flash Point | 81 (27) |
°F (°C) |
Seta |
| Solvent | Xylene | — | Supplied pre-diluted for direct application |
| Mixing Requirement | None | — | No mixing or dilution required |
| Shelf Life | 6 | months | From date of shipment; store at 70–80°F (21–27°C) in the original, unopened container |
After-Processing / Final-State Properties
Supported applied-film and drying conditions for LORD® 459X Adhesion Enhancer/Surface Modifier.
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Optimum Dry-Film Thickness | Approximately 0.1 (2.5) |
mil (µm) |
Applied by brush, dip or spray |
| Room-Temperature Air-Dry Time | 30–60 | minutes | Room temperature with good airflow |
| Oven-Dry Schedule | 5–10 | minutes | At 200–250°F (93–121°C); heat cycling generally improves adhesion |