LORD 7150A/B
Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.
Main features
- High-Strength Structural Bonding
- Primerless Bonding to Many Plastics
- Solvent-, Weathering- and Aging-Resistant Gray Cured System
Product Description
LORD® 7150-A/B Urethane Adhesive is a two-part, high-strength urethane adhesive used to bond cloth, paper, plastics, foams, rubber, painted metals and powder-coated metals. The system combines an isocyanate-based LORD® 7150-A resin with a polyol-based LORD® 7150-B curative and can be cured at room temperature or with elevated heat for faster processing. After cure, it forms a gray adhesive system with resistance to solvents, weathering and aging.
Key Features
- Broad substrate capability for cloth, paper, plastics, foams, rubber, painted metals and powder-coated metals.
- High-strength plastic bonding without crazing, attacking or reducing the strength of the plastic substrate.
- Reduced priming requirements for many plastics, helping lower material and labor requirements.
- Solvent-, weathering- and aging-resistant cured performance with no VOC content and no ozone-depleting chemicals.
Applications / Suitable for
- Plastic and foam assemblies
- Rubber bonding
- Cloth and paper laminations
- Painted-metal and powder-coated-metal assemblies
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Thermal Properties
Additional Information
As-Supplied / Before-Processing Properties
Typical component and mixed-system properties for LORD® 7150-A/B Urethane Adhesive. Values are typical and are not intended for specification purposes.
| Property | 7150-A Resin | 7150-B Curative | Mixed System | Method / Condition |
|---|---|---|---|---|
| Composition | Isocyanate-based resin | Polyol-based curative | Two-part urethane | Product description |
| Appearance | Black liquid | White liquid | — | Typical |
| Viscosity | 3,000–16,000 cP | 41,500–65,500 cP | — | At 77°F (25°C); resin: Brookfield LVT, Spindle 4, 30 rpm; curative: Brookfield HA, Spindle 6, 20 rpm |
| Density | 12.4–12.7 lb/gal (1486–1522 kg/m³) |
10.9–11.4 lb/gal (1306–1366 kg/m³) |
— | Typical |
| Flash Point | >200°F (>93°C) |
>200°F (>93°C) |
— | Closed cup |
| Mix Ratio | 1 part | 2 parts by volume 1.78 parts by weight |
1:2 by volume 1:1.78 by weight |
Resin to curative |
| Solids Content | — | — | 100% | Mixed adhesive |
| Working Time | — | — | 5–10 minutes | At 75°F (24°C) |
| Purge Time | — | — | 3 minutes | At 77°F (25°C) |
| Time to Handling Strength | — | — | 2–3 hours | At 73°F (23°C) |
| Shelf Life | 6 months | 6 months | — | Store at 65–85°F (18–30°C) in a clean, dry environment in the original, unopened container |
After-Processing / Final-State Properties
Supported cure and final-state characteristics for LORD® 7150-A/B Urethane Adhesive. Values are typical and are not intended for specification purposes.
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Full Cure Time | 24 | hours | At room temperature, 77°F (25°C); elevated temperatures accelerate cure |
| Cured Appearance | Gray | — | Typical |
| VOC Content | 0 | g/L | Documented formulation characteristic |