MOLYKOTE 112

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE 112

Main features

  • Up to 232 deg C Service
  • Oil, Acid, and Alkali Resistance
  • Low-Volatility Joint Sealing

Product Description

MOLYKOTE® 112 High Consistency Valve Sealant is a stiff, nonmelting silicone grease used primarily as a robust valve lubricant and sealant. Formulated with polydimethyl silicone fluids and an inert amorphous silica filler, it is designed for demanding environments that require a high degree of mechanical stability. It maintains its consistency without carbonizing, melting, or hardening during prolonged exposure to elevated temperatures up to 232°C (450°F).

Key features

  • Extreme temperature stability: Serviceable from -40°C to 232°C (-40°F to 450°F) without melting, hardening, or carbonizing.
  • Harsh environment resistance: Highly resistant to water, most aqueous solutions of inorganic salts, dilute acids, alkalis, and many organic compounds.
  • Low volatility: Features very low vapor pressure, making it an excellent sealer for high vacuum or pressure systems.

Applications / Suitable for

  • Lubricating valves, O-rings, and plug-valves in chemical processing
  • Sealing synthetic rubber or plastic parts in vacuum and pressure systems
  • Lubricating mechanical devices like flow meters, fire extinguisher valves, and optical equipment
Product Family

MOLYKOTE 112

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Polydimethyl silicone fluids and silica filler - Silicone grease
Appearance White-translucent / off-white - Grease / Paste (CTM 0176)
Unworked Penetration 215 - -
Worked Penetration 230 - 60 strokes, maximum
Worked Penetration 240 - 100,000 strokes
Specific Gravity 1.1 - at 25°C (77°F) (CTM 0022)
Melting Point None - -
Flash Point > 101 °C Closed cup (> 214 °F)
Shelf Life 60 months From date of manufacture
Technical properties

After-processing / in-service properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Service Temperature Range -40 to 232 °C (-40 to 450 °F)
Bleed 0.03 % 24 hours at 200°C (392°F) (CTM 0033A)
Evaporation 0.8 % 24 hours at 200°C (392°F) (CTM 0033A)
Water Spray-Off 3.0 % ASTM D4049
Dielectric Constant 2.93 - at 100 Hz (CTM 0112)
Dielectric Constant 2.92 - at 100 kHz (CTM 0112)
Dissipation Factor < 0.0001 - at 100 Hz (CTM 0112)
Dissipation Factor < 0.004 - at 100 kHz (CTM 0112)
Dielectric Strength 490 volts/mil 50 mil gap (CTM 0114)
Volume Resistivity 2.9x10^15 ohm-cm at 23°C (73°F)
Arc Resistance 122 seconds CTM 0171