MOLYKOTE 41

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE 41

Main features

  • Silicone Oil Base and Carbon Black Thickener
  • 20 to 290 deg C Service Range
  • Water and Oxidation Resistance

Product Description

MOLYKOTE® 41 Extreme High Temperature Grease is an NLGI 2 silicone grease formulated with a silicone oil base fluid and a carbon black thickener. Designed for extreme operating environments, this black grease provides superior thermal stability and does not melt, even at high temperatures. It is ideal for lubricating bearings and components in high-temperature applications such as oven conveyors, kiln dollies, and molten salt evacuation pumps.

Key features

  • High-temperature stability: Operates effectively across a service temperature range of -20°C to 290°C and features no drop point, preventing melting at elevated temperatures.
  • Environmental resistance: Delivers superior oxidation resistance and excellent water resistance, highlighted by a low water washout of 0.5% (38°C/1 hour).
  • Clean formulation: Manufactured without intentional polytetrafluoroethylene (PTFE) or per- and polyfluoroalkyl substances (PFAS).

Applications / Suitable for

  • Oven conveyors, kiln dollies, and molten salt evacuation pumps
  • Steam turbine regulator links and knife-edge power breakers
  • Note: Do not use on painted surfaces or on steel bearings under high loads
Product Family

MOLYKOTE 41

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Silicone oil, carbon black, corrosion inhibitor - Contains zinc naphthenate
Appearance Black[cite: 40, 41] - Grease[cite: 40]
NLGI Class 2 - -
Base Oil Viscosity 316 mm²/s at 25°C
Worked Penetration 260 to 300 mm/10 Worked 60 times (JIS K 2220)
Density 1.05 - 1.1[cite: 40, 41] g/cm³ Value varies between SDS relative density and TDS reporting[cite: 40, 41]
Flash Point 302[cite: 40] °C[cite: 40] Closed cup[cite: 40]
Usable Life 60 months From date of production when stored unopened in a cool, dark place
Technical properties

After-processing / in-service properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Service Temperature Range -20 to 290 °C -
Drop Point None °C JIS K 2220
Bleed 4.0 % 150°C/24 hours (MIL S 8660)
Evaporation 1.0 % 150°C/24 hours (MIL S 8660)
Water Washout 0.5 % 38°C/1 hour (JIS K 2220)
Four Ball Weld Load 1,500 N 1,500 rpm/1 minute (ASTM D2596)
Maximum Dn Value 75,000 mm/minute -