MOLYKOTE 557

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

MOLYKOTE 557

Main features

  • Clear Nonstaining Wax-Like Film
  • 0.07 Coefficient of Friction
  • Federal Meat/Poultry Program Authorization

Product Description

MOLYKOTE® 557 Silicone Dry Film Lubricant is an extreme-pressure, wax-like dry-film lubricant supplied in a solvent carrier (available as a bulk liquid or aerosol spray). Once applied, the solvent evaporates to leave a nearly transparent, clear wax film that adheres tenaciously to surfaces in both solid and fluid states. It provides exceptional release properties and heavy-duty lubrication, effectively reducing friction, wear, stick-slip, and metal seizure in demanding manufacturing and metalworking operations.

Key features

  • Clean and nonstaining: Dries to a colorless film that will not stain paper or fabrics, and is formulated without intentional polytetrafluoroethylene (PTFE) or per- and polyfluoroalkyl substances (PFAS).
  • Extreme-pressure performance: Protects heavily loaded tracks, cams, slides, and cutting tools with a four-ball weld load capacity of 1,200 N.
  • Industry authorized: Authorized for use in official establishments operating under the Federal Meat and Poultry Inspection Program (formerly USDA H2 ratings) where there is no possibility of food contact.

Applications / Suitable for

  • Metalworking operations: extruding, deep drawing, spinning, and increasing the life of slitter-blades, taps, dies, and drills
  • Lubricating heavily loaded bearings, slides, cams, adjusting screws, guides, and ways in machine shops
  • Reducing sticking and product contamination on conveyors, knives, and handling equipment in the textile, paper, woodworking, rubber, and plastic industries
Product Family

MOLYKOTE 557

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Waxlike lubricant in solvent carrier - Bulk solvent is naphtha
Appearance / Color Clear / Colourless - Supplied as liquid or aerosol spray
Specific Gravity (Bulk Liquid) 0.77 - CTM 0137A
Relative Density (Aerosol) 0.8 - Water = 1
Flash Point (Bulk Liquid) 39 °C (102°F) Bulk form only
Drying Time 30 minutes -
Usable Life (Bulk Liquid) 60 months Stored at or below 25°C (77°F) from date of manufacture
Usable Life (Aerosol Spray) 24 months Stored at or below 25°C (77°F) from date of manufacture
Technical properties

After-processing / in-service properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Appearance (As Applied) Clear wax film - After solvent evaporation
Service Temperature Range -40 to 43 °C (-40 to 110 °F) Estimated based on formulation
Melting Range 32 to 46 °C (90 to 115 °F)
Coefficient of Friction 0.07 - Tested on Falex LFW-4 Press Fit tester, steel vs. steel
Press Fit Performance No stick-slip - Falex LFW-4 Press Fit tester, steel vs. steel, Rc60, 12,000 psi
Four Ball Weld Load 1,200 N ASTM D2596
Four Ball Wear Scar 0.85 mm Fed Std 791a, Method 6514.1