MOLYKOTE 7400

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

MOLYKOTE 7400

Main features

  • Water-Based MoS2/Graphite Dry-Film Lubricant
  • High Load-Carrying Capacity
  • Air-Curing Lubricant Coating

Product Description

MOLYKOTE® 7400 Anti-Friction Coating is an environmentally friendly, water-based, air-curing dry film lubricant completely free from flammable solvents. Formulated as a dark gray liquid containing solid lubricants like molybdenum disulfide and graphite within an organic binder, it dries to provide a permanent, non-soiling lubricating film. It excels in metal-to-metal applications involving high loads and slow-to-moderately fast movements, serving as an excellent alternative where the use of traditional oils or greases is restricted due to design or contamination risks.

Key features

  • Solvent-free formulation: Water-based chemistry eliminates flammable solvents, improving workplace safety while providing a low coefficient of friction.
  • High load capacity: Withstands extreme contact pressures, exhibiting a Falex load-carrying capacity of 11,300 N on phosphatized surfaces.
  • Rapid air curing: Offers fast, flexible curing options—achieving a fully cured film in just 40 minutes at room temperature (23°C) or in 5 minutes at 90°C.

Applications / Suitable for

  • Maintenance-free, permanent, and non-soiling lubrication of highly stressed friction combinations
  • Improving the running-in of gearboxes, sliding bearings, sliding guides, and car transmission shafts
  • Lubricating threaded sleeves of car seat adjusting mechanisms and cold working of steel
Product Family

MOLYKOTE 7400

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Solid lubricants, organic binder, water, inhibitors, stabilizers - Contains molybdenum disulfide and graphite
Physical State / Appearance Dark gray / Grey - Liquid
Viscosity (Efflux Time) 24 s at 20°C (DIN4 cup) (DIN 53211/4)
Kinematic Viscosity 24 mm²/s at 25°C (77°F)
Density 1.16 - 1.165 g/ml at 20°C (DIN 53217/2). Value varies between SDS Relative Density and TDS reporting
Nonvolatile Content 30 % CTM 02421
pH 6 - 8 - at 20°C (CTM 0007 A). Value varies between SDS and TDS
Flash Point > 100 °C Closed cup (> 212 °F)
Shelf Life 12 months Stored between 1°C and 30°C in unopened containers
Technical properties

After-processing / in-service properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Recommended Dry-Film Thickness 5 to 20 µm -
Drying Time 15 minutes at 20°C
Curing Time 40 minutes at 23°C (object temperature)
Curing Time (Alternative) 10 minutes at 50°C (object temperature)
Curing Time (Alternative) 5 minutes at 90°C (object temperature)
Service Temperature Range -70 to +200 °C -
Falex Load-Carrying Capacity 11,300 (p) / 7,900 (s) N ASTM D2625 (p = phosphate, s = sandblasted surface pretreatment)
LFW-1 Wear (Rotating) 343 N Revolutions x1,000 to µ=0.1 (F=2,860 N, n=72 rpm, v=7.9 m/min, phosphatized) (ASTM D2714)
LFW-1 Wear (Oscillating) 76 N Oscillations x1,000 to µ=0.08 (F=900 N @ 89.5 osc/min, phosphatized)
Fretting Corrosion (Deyber Test) 10 x 10^6 - -