MOLYKOTE G-0052

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE G-0052

Main features

  • FDA 21 CFR 178.3570 Compliance
  • 6,080 N Four-Ball Weld Load
  • Water-Resistant Grease Lubrication

Product Description

MOLYKOTE® G-0052 FM White E.P. Bearing Grease is a high-performance, mineral-oil-based lubricant thickened with an aluminum complex. Specially formulated for the food and beverage industry, this white, NLGI 2 multipurpose grease is fortified with extreme pressure (EP) and anti-wear (AW) additives to protect highly loaded mechanical components. It provides an excellent lubrication solution where an NSF H1 status lubricant is required or when the environment must remain free of black particle contamination.

Key features

  • Food-grade compliance: Meets FDA Regulation 21 CFR 178.3570, holds the NSF H1 classification for incidental food contact, and is Kosher approved.
  • High load capacity: Effectively protects bearings and gears under heavy loads, demonstrating a high four-ball weld load of 6,080 N (620 KG).
  • Robust environmental resistance: Provides good resistance to water washout and is broadly compatible with many plastics and elastomers used in food processing machinery.

Applications / Suitable for

  • Multipurpose lubrication of mechanical components in food and beverage processing facilities
  • Anti-friction bearings and plain bearings
  • Chains, gears, and sliding mechanisms
Product Family

MOLYKOTE G-0052

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Mineral oil, aluminum complex thickener, EP/AW additives - Contains zinc oxide
Appearance / Color White - Grease
NLGI Consistency Class 2 - DIN 51 818
Penetration 280 mm/10 ASTM D217
Density 0.89 - 1.08 g/ml at 20°C (ISO 2811).
Base Oil Viscosity 99 cSt at 40°C (ASTM D445)
Flash Point > 200 °C Closed cup
Usable Life 60 months From date of production when stored at or below 32°C (90°F) in unopened containers
Technical properties

After-processing / in-service properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Service Temperature Range -17 to +150 °C (0 to +302 °F)
Drop Point 269 °C (516 °F) (ASTM D2265)
Four-Ball Weld Load 6,080 N (620 KG) (ASTM D2596)
Four-Ball Wear Scar 0.9 mm ASTM D2266
Water Washout 10 % at 175°F (ASTM D1264)
Oil Bleed <= 5 % max 24 hrs @ 100°C (Fed 791)
Oil Evaporation <= 2.0 % max 24 hrs @ 100°C (Fed 791)