MOLYKOTE G-1067
Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses
Main features
- Low-Friction Plastic-Compatible PAO Grease
- 50 to 120 deg C Service Range
- Automotive Lubrication Applications
Product Description
MOLYKOTE® G-1067 Grease is a white, synthetic lubricating grease formulated with a polyalphaolefin (PAO) base oil, a lithium soap thickener, and white solid lubricants. Specifically designed for automotive body and plastic components, this smooth, buttery grease provides exceptional lubricity and noise-damping properties. It excels in applications involving plastic-to-metal and plastic-to-plastic interfaces, particularly glass-fiber-reinforced plastics (GFRP).
Key features
- Excellent plastic compatibility: Highly compatible with most plastics, providing low friction and reduced noise at steel/GFRP interfaces.
- Broad temperature range: Delivers reliable lubrication across a wide service temperature range of -50°C to 120°C (-45°F to 257°F).
- Clean formulation: Formulated without intentional polytetrafluoroethylene (PTFE) or per- and polyfluoroalkyl substances (PFAS).
Applications / Suitable for
- Automotive rail parts, including sunroof and moonroof slides
- Lubrication of glass-fiber-reinforced plastic (GFRP) parts against steel or other plastics
- Industrial assembly and appliance slides, guides, and linear drives
TDS, SDS & Technical Documents
Technical Specifications
No specifications available.
Additional Information
As-supplied / before-processing properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical Composition | Polyalphaolefin (PAO) oil, lithium soap thickener, white solid lubricants | - | Organic grease |
| Appearance / Color | White / Off-white to beige | - | Smooth, buttery grease |
| NLGI Consistency Class | 2 | - | - |
| Worked Penetration | 302 - 342 | mm/10 | Worked 60 strokes (JIS K 2220 / ASTM D217) |
| Base Oil Viscosity | 31.2 | cSt | at 40°C |
| Relative Density | 0.83 | - | Water = 1 |
| Flash Point | > 100 | °C | (212°F) Seta closed cup |
| Shelf Life | 36 | months | Stored closed below 40°C in original containers |
After-processing / in-service properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Service Temperature Range | -50 to 120 | °C | (-45 to 257°F) |
| Dropping Point | 210 | °C | (410°F) (JIS K 2220 / ASTM D566) |
| Bleed | 0.0 | % | 24 hrs at 100°C (JIS K 2220 / ASTM D566) |
| Evaporation | 0.1 - 0.4 | % | 22 hrs at 99°C (JIS K 2220 / ASTM D566) |
| Copper Corrosion Test | 1a | - | 24 hrs at 100°C (JIS K 2220) |
| Four Ball Wear Scar | 0.67 | mm | 1,200 rpm, 392 N, 1 hr (75°C) (ASTM D2266) |
| Low-Temperature Torque (Starting) | 46 | mN*m | at -40°C (JIS K 2220 / ASTM D1478) |
| Low-Temperature Torque (Running) | 22 | mN*m | at -40°C (JIS K 2220 / ASTM D1478) |