MOLYKOTE G-1502FM
Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses
Main features
- Oil and Water Resistance
- FDA 21 CFR 178.3570 Compliance
- 40 to 149 deg C Service Range
Product Description
MOLYKOTE® G-1502 FM Synthetic Bearing & Gear Grease is a high-performance, white, food-grade grease formulated with an aluminum complex thickener, a 100% polyalphaolefin (PAO) synthetic base oil, and a carefully selected combination of lubricating solids. Designed for incidental food contact applications, this NLGI 2-3 grease is highly tacky, providing exceptional adhesion and robust resistance to water washout and spray-off. It is ideal for lubricating chains, open gears, valves, and sprockets in food processing environments where moisture is prevalent or grease sling-off cannot be tolerated.
Key features
- Food-grade and safe formulation: NSF H1 approved and meets FDA 21 CFR 178.3570 regulations for incidental food contact. It is entirely free of intentional allergens, GMOs, animal-derived content, PTFE, and PFAS.
- Exceptional water and sling resistance: The tacky consistency delivers powerful adhesion and resistance to water wash-off, ensuring the lubricant stays precisely where it is needed.
- High load and wear protection: Provides outstanding extreme-pressure and anti-wear capabilities with a four-ball weld load of 400 kg and a Timken OK load of 50 lb (110 kg).
Applications / Suitable for
- Chains, cams, open gears, valves, and sprockets
- Food and beverage applications where a highly adhesive, tacky grease is required
- Environments where water wash-off is problematic or sling-off must be avoided
Technical Specifications
No specifications available.
Additional Information
As-supplied / before-processing properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical Composition | 100% PAO base oil (ISO 220), aluminum complex thickener, lubricating solids | - | Contains 5-10% white mineral oil |
| Appearance / Color | White to off-white | - | Grease |
| NLGI Consistency Class | 2 - 3 | - | - |
| Base Oil Viscosity | 220 | cSt | at 40°C (104°F) (ASTM D445) |
| Base Oil Viscosity | 25.2 | cSt | at 100°C (212°F) (ASTM D445) |
| Viscosity Index | 145 | - | ASTM D2270 |
| Unworked Penetration | 255 | mm/10 | at 25°C (77°F) (ASTM D217) |
| Worked Penetration | 250 | mm/10 | at 25°C (77°F), W/60 (ASTM D217) |
| Relative Density | 0.85 | - | Water = 1 |
| Flash Point | 260 | °C | Closed cup (500°F) |
| Shelf Life | 60 | months | From date of production when stored unopened at 0°C to 35°C (32°F to 95°F) |
After-processing / in-service properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Service Temperature Range | -40 to 149 | °C | (-40 to 300°F) Estimated |
| Dropping Point | 260 | °C | (500°F) (ASTM D556) |
| Four-Ball Wear Scar | 0.60 | mm | 40 kg, 1,200 rpm, 75°C (167°F) max (ASTM D2266) |
| Four-Ball Weld Load | 400 | kg | ASTM D2596 |
| Timken OK Load | 110 | kg | (50 lb) (ASTM D2509) |
| Rust Test | PASS | - | ASTM D1743 |
| Copper Corrosion | 1B | - | ASTM D4048 |
| Food Grade Compliance | Pass | - | NSF H1, FDA 21 CFR 178.3570 |
| Allergen / GMO Content | None | - | No intentional or known GMO, animal-derived content, or Annex II allergens |