MOLYKOTE G-3407
Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses
Main features
- -40 to 200 deg C Service Range
- Brake-Caliper Guide-Pin Lubrication
- 120-Hour No-Rust Test Result
Product Description
MOLYKOTE® G-3407 Caliper Pin Grease is a light-green synthetic grease formulated with polyalkylene glycol (PAG) base oil and a lithium-complex thickener for automotive brake-caliper guide pins and other supported metal-to-metal contacts. Its documented service-temperature range is -40°C to 200°C. Product-specific test data include less than 5% bleed and evaporation after 24 hours at 150°C, less than 5% water washout at 80°C, no rust after 120 hours in ASTM B117 testing, and bounded EPDM volume- and hardness-change limits after 72 hours at 150°C. Apply to clean contact surfaces using a clean brush or manual or automated dispensing equipment, and confirm compatibility with the exact elastomer and assembly conditions before use.
Key features
- Caliper guide-pin lubrication: PAG-based grease intended for automotive brake-caliper mounting pins and supported metal-to-metal pairings.
- Wide service-temperature range: Documented for operation from -40°C to 200°C.
- High-temperature retention data: Less than 5% bleed and less than 5% evaporation after 24 hours at 150°C.
- EPDM compatibility evidence: Maximum 8% volume change and maximum 8 Shore A hardness change after 72 hours at 150°C under the stated test.
- Water and corrosion test results: Less than 5% water washout at 80°C and no rust after 120 hours in ASTM B117 testing.
Applications / Suitable for
- Automotive brake-caliper guide and mounting pins
- Supported metal-to-metal sliding contacts in brake-caliper assemblies
- Manual or automated grease-dispensing processes for caliper-pin lubrication
TDS, SDS & Technical Documents
Technical Specifications
No specifications available.
Additional Information
MOLYKOTE® G-3407 Caliper Pin Grease
A PAG-based, lithium-complex synthetic grease for automotive brake-caliper guide pins and supported metal-to-metal contacts. The product combines a -40°C to 200°C service range with high-temperature retention, water-washout, corrosion, low-temperature torque, and EPDM compatibility data for application-specific evaluation.
MOLYKOTE® G-3407 Caliper Pin Grease is supplied as a light-green synthetic grease for caliper guide-pin lubrication.
As-supplied grease properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Light green | — | As supplied |
| Penetration, unworked | 260–310 | mm/10 | CTM 0191 / ASTM D217 |
| Penetration, worked | 260–310 | mm/10 | CTM 0191 / ASTM D217 |
| Specific gravity | 1.00 ± 0.1 | g/mL | CTM 0044 at 25°C |
| Dropping point | >250 | °C | ASTM D566; test result, not a service-temperature limit |
Typical values are not specification limits.
Service performance and compatibility
| Property | Result | Unit | Method / condition |
|---|---|---|---|
| Bleed | <5 | % | ASTM D6184; 24 h at 150°C |
| Evaporation | <5 | % | CTM 0033A; 24 h at 150°C |
| Corrosion protection | No rust | — | ASTM B117; 120 h |
| Low-temperature torque, starting | 2,000 max. | gf·cm | ASTM D1478 at -20°C |
| Low-temperature torque, running | 800 max. | gf·cm | ASTM D1478 at -20°C |
| Water washout | <5 | % | ASTM D1264 at 80°C |
| EPDM volume change | 8 max. | % | CTM 0130 / ASTM D4289; 72 h at 150°C |
| EPDM hardness change | 8 max. | Shore A | CTM 0130 / ASTM D4289; 72 h at 150°C |
Results are specific to the listed methods and conditions. EPDM compatibility should not be generalized to every elastomer grade, formulation, aged component, or mixed-lubricant condition.
Prepare and dispense for caliper guide-pin lubrication
Apply the grease to clean contact surfaces using conventional grease-application methods. Control the amount and distribution according to the caliper design, component geometry, elastomer system, and validated assembly process.
The final visual should show clean guide-pin preparation and controlled grease placement without implying a universal fill quantity.
Store at or below 40°C in the original unopened container. Usable life is 60 months from the date of production under the stated storage condition. Review the current safety data and container label before handling, use adequate ventilation, and keep the product away from strong oxidizing agents.
Evaluate MOLYKOTE® G-3407 for your brake-caliper guide-pin system
Krayden can help review caliper geometry, operating temperature, elastomer grade, existing lubricant, water exposure, dispensing method, and validation requirements. Contact us to discuss product fit, samples, technical data interpretation, or an application-specific evaluation plan.