MOLYKOTE G-4500FM

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE G-4500FM

Main features

  • 40 to 150 deg C Service Range
  • 18 kg Four-Ball Weld Load
  • NLGI 2 PAO/Aluminum-Complex Grease

Product Description

MOLYKOTE® G-4500 FM Multi-Purpose Synthetic Grease is a white, NLGI 2 grease based on a fully synthetic PAO base oil, an aluminum-complex thickener, and white solid lubricants including PTFE. It is documented for rolling-element and plain bearings, pivot pins, cams, guides, ways, drive screws, gears, splines, chains, and sliding mechanisms, including machinery used in food processing. The approximate service range is -40°C to 150°C. Typical evaluation data include 0.9 N·m low-temperature torque at -40°C, a four-ball weld load above 3,100 N, a 0.5 mm four-ball wear scar, and an estimated Dn value of 325,000. Confirm the exact plastic, elastomer, regulatory, load, speed, and dispensing requirements for the intended assembly.

Key features

  • Synthetic grease system: PAO base oil with an aluminum-complex thickener and white solid lubricants, including PTFE.
  • Operating-temperature range: Approximate service range of -40°C to 150°C.
  • Load and wear test data: More than 3,100 N four-ball weld load, more than 18 kg Timken OK load, and a 0.5 mm wear scar under the stated test conditions.
  • Low-temperature evaluation: ASTM D4693 torque result of 0.9 N·m at -40°C.
  • Retention data: Typical oil bleed of 3.1 wt% and evaporation of 0.4 wt% after 24 hours at 100°C.
  • Material-selection context: Supplier literature identifies compatibility with many plastics and elastomers; verify the exact grade and exposure conditions before use.

Applications / Suitable for

  • Rolling-element and plain bearings
  • Gears, drive screws, splines, cams, guides, and ways
  • Pivot pins, chains, and sliding mechanisms
  • Machine elements involving selected plastic, rubber, or metal interfaces
  • Food-processing machinery mechanisms, subject to confirmation of applicable regulatory and incidental-contact requirements

Technical Specifications

No specifications available.

Additional Information

Multi-purpose synthetic grease

MOLYKOTE® G-4500 FM Multi-Purpose Synthetic Grease

A white NLGI 2 grease using PAO base oil, an aluminum-complex thickener, and white solid lubricants for bearings, gears, drive screws, guides, chains, and other machine elements. Its approximate -40°C to 150°C range is supported by condition-specific low-temperature torque, load, wear, bleed, evaporation, and bearing-speed data.

NLGI 2 PAO / aluminum complex -40°C to 150°C 100 cSt at 40°C Estimated Dn 325,000
Approved product image showing the exact MOLYKOTE G-4500 FM Multi-Purpose Synthetic Grease package and label.

MOLYKOTE® G-4500 FM is a white, fully synthetic multi-purpose grease for machine-element lubrication.

As supplied

Grease composition, consistency, and viscosity

Grease system
PAO / aluminum complex
Fully synthetic PAO base oil with an aluminum-complex thickener and white solid lubricants.
Consistency
NLGI 2
Worked penetration is reported separately at 265–295 mm/10 under ASTM D217.
Base-oil viscosity
100 cSt at 40°C
A second value of 14.4 cSt at 100°C describes the temperature-dependent base-oil viscosity.
Property Value Unit Method / condition
Color White — As supplied
NLGI consistency class 2 — DIN 51818
Worked penetration at 25°C 265–295 mm/10 ASTM D217; 60 strokes
Base-oil viscosity at 40°C 100 cSt ASTM D445
Base-oil viscosity at 100°C 14.4 cSt ASTM D445
Specific gravity at 25°C 0.84 g/mL ISO 2811
Usable life 60 months At or below 40°C in original unopened containers

Typical values are not specification limits. NLGI grade, penetration, base-oil viscosity, and specific gravity describe different properties and should not be treated as interchangeable.

In service

Temperature, retention, load, wear, and speed data

Service temperature
-40°C to 150°C
Approximate supplier-documented range; it does not imply unchanged viscosity, wear, or life across the full range.
Four-ball weld load
>3,100 N
ASTM D2596 minimum weld-load result; this bench value is not equipment load capacity.
Bearing-speed screening
Dn 325,000
Estimated bearing inside diameter in millimeters multiplied by rotational speed in rpm.
Property Value Unit Method / condition
Approximate service-temperature range -40 to 150 °C Supplier-documented range
Dropping point >270 °C ASTM D2265; test transition, not service limit
Oil bleed 3.1 wt% FD 791-32/2; 24 h at 100°C
Oil evaporation 0.4 wt% FD 791-32/2; 24 h at 100°C
Low-temperature torque 0.9 N·m ASTM D4693; at -40°C
Four-ball wear scar 0.5 mm ASTM D2266; 40 kg, 1,200 rpm
Four-ball EP weld load >3,100 N ASTM D2596; minimum
Timken OK load >18 kg ASTM D2509
Estimated Dn value 325,000 mm·rpm Bearing inside diameter (mm) × speed (rpm)

Results are condition-specific laboratory values. The dropping point is not a continuous service limit, and the bench load and wear metrics do not define bearing, gear, or machine capacity.

Application process

Prepare and dispense the grease consistently

Apply to clean lubrication points using a clean brush, grease gun, or controlled manual or automated dispensing equipment. Grease quantity, fill level, distribution, and relubrication practice should be established for the actual component geometry and duty cycle.

Surface condition: Remove contamination and incompatible residual lubricant; apply to clean parts using tools and equipment that do not introduce debris.
Application methods: Use a clean brush, grease gun, or manual or automated dispensing equipment appropriate to the assembly.
Compatibility control: Confirm the exact plastic, elastomer, coating, and existing lubricant because similar material families and lubricant mixtures may behave differently.
Technician applying white grease with a clean grease gun or controlled dispenser to a bearing, gear, or sliding machine element.

Use controlled dispensing and the equipment manufacturer’s specified grease quantity and fill practice.

Storage and Handling

Usable life is 60 months from the date of production when stored at or below 40°C in the original unopened container. Keep containers properly labeled, avoid strong oxidizing agents, use adequate ventilation, and review the current safety data and container label before handling.

Applications

Multi-purpose machinery lubrication applications

Application suitability depends on the actual contact materials, load, speed, temperature, contamination, lubricant quantity, dispensing method, and maintenance practice. The contexts below reflect documented uses and available product data.

Rolling-element bearing and plain-bushing assembly in industrial machinery.
Rolling-element and plain bearings
The NLGI 2 consistency, 100 cSt base-oil viscosity at 40°C, and estimated Dn value of 325,000 provide selection data for bearing applications. Confirm bearing type, speed, load, temperature, fill quantity, sealing, and relubrication requirements.
Metal gear, drive screw, spline, cam, guide, and sliding mechanism requiring grease lubrication.
Gears, screws, splines, and sliding mechanisms
Documented applications include gears, drive screws, splines, cams, guides, ways, and other sliding machine elements. Four-ball and Timken results provide bounded bench-test context for load and wear evaluation without defining equipment capacity.
Bearing, chain, gear, and sliding mechanism installed in food-processing or packaging machinery.
Food-processing machinery mechanisms
Supplier literature documents use in bearings, gears, chains, and sliding mechanisms in food-processing machinery. Confirm the exact incidental-contact registration, application boundary, facility requirements, and contamination controls before specification.
Next steps

Evaluate MOLYKOTE® G-4500 FM for your machinery lubrication system

Krayden can help review bearing speed, contact load, temperature, plastic or elastomer compatibility, grease quantity, dispensing equipment, existing-lubricant compatibility, food-machinery application boundaries, and the test data most relevant to your qualification plan.