MOLYKOTE G-4700
Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses
Main features
- Extreme-Load Bearing Lubrication
- PAO Synthetic Base Oil and Lithium Complex Thickener
- Industrial Plastic/Elastomer Compatibility
Product Description
MOLYKOTE® G-4700 Extreme Pressure Synthetic Grease is a high-performance, light-consistency synthetic grease formulated with a polyalphaolefin (PAO) base oil, a lithium complex thickener, and fortified with molybdenum disulfide (MoS₂) solid lubricants. Engineered to handle extreme loads, vibration, and shock loading, it offers a higher load-carrying capacity, greater wear resistance, and longer service life than conventional petroleum-based lubricants.
Key features
- Extreme-pressure performance: Designed specifically to withstand extreme loads and shock loading, boasting a high four-ball weld load of 3,700 N.
- Wide operating range & compatibility: Delivers reliable lubrication across a broad temperature range of -40°C to 177°C (-40°F to 350°F) and provides good compatibility with most industrial plastics and elastomers.
- Industry approvals: Meets Cincinnati Machine P-64 and NLGI GC-LB specifications. Formulated without intentional polytetrafluoroethylene (PTFE) or per- and polyfluoroalkyl substances (PFAS).
Applications / Suitable for
- Rolling element and plain bearings
- Pivot pins, cams, guides, and ways
- Drive screws, gears, splines, and other heavily loaded machine elements
TDS, SDS & Technical Documents
Technical Specifications
No specifications available.
Additional Information
As-supplied / before-processing properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical Composition | PAO base oil, lithium complex thickener, MoS2 | - | Organic grease |
| Appearance / Color | Black / Dark grey | - | Grease |
| NLGI Consistency Class | 2 | - | DIN 51 818 |
| Worked Penetration | 265-295 | mm/10 | at 25°C (77°F), W/60 (ASTM D217) |
| Base Oil Viscosity (40°C) | 150 | cSt | ASTM D445 |
| Base Oil Viscosity (100°C) | 20 | cSt | ASTM D445 |
| Specific Gravity / Relative Density | 0.87 | g/ml | at 25°C (77°F) (ISO 2811) |
| Flash Point | > 230 | °C | (446°F) Closed cup |
| Usable Life | 60 | months | Stored at or below 35°C (95°F) in original unopened containers |
After-processing / in-service properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Service Temperature Range | -40 to 177 | °C | (-40 to 350°F) Approximate |
| Dropping Point | > 285 | °C | (> 545°F) (ASTM D2265) |
| Low-Temperature Torque | .024 | Nm | at -40°C (-40°F) (ASTM D4693) |
| Four-Ball Wear | 0.64 | mm | 40 kg, 1,200 rpm (ASTM D2266) |
| Four-Ball EP Weld Load | 3,700 | N | Minimum (ASTM D2596) |
| Dn Value | 350,000 | mm/min | Estimated (bearing ID x rpm) |
| Oil Bleed | 3.9 | wt% | 24 hours at 100°C (212°F) (FD 791-32/2) |
| Oil Evaporation | 0.44 | wt% | 24 hours at 100°C (212°F) (FD 791-32/2) |