MOLYKOTE L-1468 FM
Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other
Main features
- ISO VG 68 PAO Chain Oil
- Freezer-Chain Anti-Wear Lubrication
- NSF H1 Registration
Product Description
MOLYKOTE® L-1468 FM Synthetic Freezer Chain Oil is an ISO VG 68 synthetic chain lubricant based on polyalphaolefin oil. Developed for low-temperature chain applications, it incorporates rust, oxidation, antiwear, corrosion-inhibiting, tackifier, and pour-point-depressant additives. The amber oil supports dependable lubrication across a broad temperature range while helping the lubricant remain on chain surfaces. It is NSF H1 registered for applications where incidental food contact may occur, making it suitable for freezer chains and food-processing equipment when used in accordance with applicable registration and equipment requirements.
Key features
- Low-temperature chain lubrication: Formulated for freezer chains and other low-temperature chain-drive applications.
- Synthetic PAO technology: Provides oxidation resistance and viscosity stability across a broad temperature range.
- Multi-functional additive package: Contains rust, oxidation, antiwear, corrosion-inhibiting, tackifier, and pour-point-depressant additives.
- Chain retention: The tackifier supports adhesion of the lubricant to chain components.
- Food-processing suitability: NSF H1 registered for incidental food-contact applications.
- Formulation statement: Contains no intentionally added PTFE or PFAS.
Applications / Suitable for
- Freezer and cold-storage conveyor chains
- Low-temperature chain-drive systems
- Food-processing machinery chains
- Chain applications requiring an NSF H1 registered ISO VG 68 lubricant
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Supplier-documented as-supplied characteristics of MOLYKOTE® L-1468 FM Synthetic Freezer Chain Oil.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product type | Synthetic chain oil | — | MOLYKOTE® oil |
| Base-oil technology | Polyalphaolefin | — | PAO synthetic base oil |
| ISO viscosity grade | 68 | — | ISO VG classification |
| Viscosity index | 131 | — | Supplier-listed product detail |
| Color | Amber | — | As supplied |
| Additive system | Rust, oxidation, antiwear, tackifier, pour-point depressant and corrosion inhibitors | — | Supplier-described additive package |
| NSF registration | H1 | — | Incidental food-contact lubricant |
After-application / in-service properties
Supplier-documented performance characteristics relevant to chain lubrication under service conditions.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Recommended temperature range | −50 to 120 | °C | DuPont industrial lubricant selector guide; oiled chains |
| Low-temperature performance | Suitable for freezer-chain service | — | Supplier-listed product function |
| Corrosion protection | Good | — | Supplier-listed qualitative performance benefit |
| Oxidation resistance | Good | — | Supplier-listed qualitative performance benefit |
| Lubricant retention | Tackified | — | Additive-supported adhesion to chain surfaces |