MOLYKOTE LONGTERM 2 PLUS
Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses
Main features
- 3,800 N Four-Ball Weld Load
- Heavily Loaded Metal-to-Metal Components Protection
- 25 to 110 deg C Service Range
Product Description
MOLYKOTE® Longterm 2 Plus Extreme Pressure Bearing Grease is a black, mineral-oil-based, lithium-soap grease for highly loaded metal-to-metal components operating at slow to medium-fast speeds. The NLGI Grade 2 formulation contains solid lubricants and extreme-pressure additives that provide wear protection under mixed-friction conditions. It is designed for long-term lubrication of bearings, spline profiles, clutches, guides, slides, and power screw drives, including equipment exposed to moisture, fretting corrosion, or groove formation. The grease can be applied manually or through compatible central lubrication systems and has a normal service-temperature range of −25°C to 110°C.
Key features
- High load-carrying capacity: Provides a typical four-ball weld load of 3,800 N.
- Mixed-friction wear protection: Uses solid lubricants and extreme-pressure additives to protect loaded metal contacts.
- Long-term lubrication: Formulated for extended lubrication of suitable components and operating conditions.
- Good adhesion: Contains an adhesion improver to help retain the grease on lubricated surfaces.
- Corrosion and fretting protection: Suitable for components exposed to moisture or oscillating contact.
- Central-system application: Can be applied by brush, spatula, automatic lubrication device, or compatible central lubrication system.
Applications / Suitable for
- Rolling-element and plain bearings
- Spline profiles and clutches
- Slides, guides, tracks, bushings, and sleeves
- Power screw drives
- Motor vehicles, tractors, cranes, earth-moving machinery, conveyors, and forklift trucks
- Components exposed to moisture, fretting corrosion, or groove formation
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Typical as-supplied characteristics of MOLYKOTE® Longterm 2 Plus Extreme Pressure Bearing Grease. Values are not intended as specification limits.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Base-oil technology | Mineral oil | — | Supplier-listed composition |
| Thickener | Lithium soap | — | Supplier-listed composition |
| Solid lubricants | MoS2 and graphite | — | Current DuPont product details |
| Color | Black | — | Typical property |
| NLGI consistency class | 2 | — | DIN 51818 |
| Worked penetration | 265–295 | 0.1 mm | ISO 2137 |
| Density | 0.9 | g/mL | ISO 2811 at 20°C |
| Base-oil viscosity | 265 | mm²/s | DIN 51562 at 40°C; calculated base-oil-mixture value |
| Usable life | 60 | months | Original unopened container stored between 0°C and 40°C |
After-application / in-service properties
Typical performance characteristics of the applied grease under the stated laboratory conditions.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Service-temperature range | −25 to 110 | °C | Short periods up to 130°C |
| Drop point | ≥175 | °C | ISO 2176 |
| Four-ball weld load | 3,800 | N | DIN 51350-4 |
| Four-ball wear scar | 1.0 | mm | DIN 51350-5 under 800 N load |
| Almen-Wieland OK load | 20,000 | N | Frictional force at OK load: 3,200 N |
| FAG FE9 bearing life, F50 | 100 | h | DIN 51821-02-A; FE9, 4500/6000-110 |
| DN value | 250,000 | mm/min | Supplier-listed speed characteristic |
| Oxidation resistance | 0.3 | bar | DIN 51808; pressure drop after 100 h at 99°C |
| Corrosion protection | 0–1 | — | DIN 51802, SKF-Emcor degree of corrosion |
| Oil separation | 1.7 | % | DIN 51817 standard test |