MOLYKOTE Z-POWDER

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

MOLYKOTE Z-POWDER

Main features

  • 98% MoS2 Solid Lubricant
  • 185 to 400 deg C Service Range
  • 0.048 Coefficient of Friction

Product Description

MOLYKOTE® Z Powder is a charcoal-gray to black, free-flowing molybdenum disulfide solid lubricant for metallic contacts and lubricant-modified materials. It can be dry-burnished onto clean metal surfaces or incorporated into self-lubricating plastics, elastomers, sintered-metal parts, metalworking compounds, and brake-lining formulations. The powder is suited to heavy-load, slow-speed, press-fit, run-in, dusty, and temperature-extreme applications. With 98% typical MoS2 purity, a service-temperature range of −185°C to 400°C in atmosphere, and capability up to 1,100°C in vacuum, it supports lubrication where conventional liquid or grease films may be unsuitable.

Key features

  • High-purity solid lubricant: Contains a typical 98% molybdenum disulfide content.
  • Broad temperature capability: Supports service from −185°C to 400°C in atmosphere and up to 1,100°C in vacuum.
  • High load-carrying performance: Provides a typical Almen-Wieland OK load greater than 20,000 N.
  • Low-friction behavior: Provides a typical press-fit coefficient of friction of 0.048 under the stated test method.
  • Flexible use: Can be dry-burnished onto metal or added to plastics, elastomers, sintered metals, and lubricant formulations.
  • Extreme-environment suitability: Supports heavy-load, slow-speed, dusty, run-in, and press-fit applications.

Applications / Suitable for

  • Dry-burnished lubricating films on metallic contacts
  • Self-lubricating plastics and elastomers
  • Sintered-metal components
  • Metalworking compounds and brake-lining formulations
  • Press-fits and assembly run-in
  • Heavy-load, slow-speed, dusty, vacuum, and temperature-extreme environments
Product Family

MOLYKOTE Z-POWDER

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Product Type Product Type
Free-flowing solid-lubricant powder
Specific Gravity Specific Gravity
4.8 g/cm³ theoretical density; 1.3 g/cm³ bulk density
Thermal Properties
Operating Temperature Operating Temperature
−185°C to 400°C in atmosphere; up to 1,100°C in vacuum °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied characteristics and storage information for MOLYKOTE® Z Powder. Values are not intended as specification limits.

Property Value Unit Method / condition
Product type Solid lubricant powder — Molybdenum disulfide lubricant
Composition Molybdenum disulfide — MoS2
Appearance Charcoal gray to black — Typical property
Consistency Free-flowing powder — As supplied
MoS2 purity 98 % Typical content
Particle size, D90 <78.38 µm CTM 1392; laser method in 2-propanol
Particle size, D50 <31.59 µm CTM 1392; laser method in 2-propanol
Particle size, Fisher method 3–4 µm CTM 0268A
Theoretical density 4.8 g/cm³ Solid state
Bulk density 1.3 g/cm³ ISO 3923-2; powder state
Water/moisture content 0.02 % CTM 0262M
Usable life 60 months Original unopened bags stored at or below 20°C
Technical properties

After-application / in-service properties

Typical performance characteristics of the dry-burnished or incorporated solid lubricant under the stated conditions.

Property Value Unit Method / condition
Service-temperature range −185 to 400 °C Atmospheric service
Vacuum temperature capability Up to 1,100 °C In vacuum; application-specific
Almen-Wieland OK load >20,000 N Typical laboratory result
Coefficient of friction 0.048 µ Press-fit test
Oxidation resistance Resistant — Supplier-documented qualitative characteristic
Lubrication regime Heavy load / slow speed — Documented application context